MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Borealis BB125MO Polypropylene Copolymer
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene Copolymer

Material Notes: BB125MO is a heterophasic copolymer. This grade is a low melt flow rate grade intended for blow molding and sheet extrusion, and features extremely good process ability with improved melt strength and melt stability. As all polypropylenes, this grade shows excellent stress-cracking and chemical resistances. This polymer is one of the IMP (improved mechanical stability) grades, and is characterized by very high stiffness without any loss of impact strength even at low temperatures. Its very good organoleptic properties allows this grade to be used with any master batch without discoloring problems. Applications: corrugated boards, and industrial chemicals.

Information provided by Borealis AG

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.906 g/cc0.0327 lb/in³ISO 1183
Melt Flow  1.3 g/10 min
@Load 2.16 kg,
Temperature 230 °C
1.3 g/10 min
@Load 4.76 lb,
Temperature 446 °F
ISO 1133
 2.3 g/10 min
@Load 5.00 kg,
Temperature 190 °C
2.3 g/10 min
@Load 11.0 lb,
Temperature 374 °F
ISO 1133
 6.0 g/10 min
@Load 5.00 kg,
Temperature 230 °C
6.0 g/10 min
@Load 11.0 lb,
Temperature 446 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 9090ISO 2039-2
Tensile Strength, Yield 24.0 MPa3480 psi50mm/min; ISO 527-2
Elongation at Yield 4.0 %4.0 %50mm/min; ISO 527-2
Tensile Modulus 1.30 GPa189 ksi1mm/min; ISO 527-2
Charpy Impact, Notched 5.00 J/cm²
@Temperature 23.0 °C
23.8 ft-lb/in²
@Temperature 73.4 °F
ISO 179/1eA
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 90.0 °C194 °FISO 75-2
 
Processing PropertiesMetricEnglishComments
Middle Barrel Temperature 190 - 220 °C374 - 428 °F
Die Temperature 180 - 220 °C356 - 428 °F
Melt Temperature 180 - 220 °C356 - 428 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
PolyMirae Moplen EP440G High stiffness sheet Polypropylene Copolymer
Borealis BB213CF Polypropylene Copolymer
Borealis HB600TF Polypropylene
Borealis HC600TF Polypropylene
Borealis BC142MO Polypropylene Copolymer

PBOREA306 / 108566

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.