SE-064AN is a SEBS base thermoplastic elastomer(TPE) product. SEBS based TPEs don’t need cross-linking process and can be processed by general thermoplastic processing equipment. It has low compression set, weatherability, cold-resistance and ozone resistance. Applications: Grip, Gasket etc. Information provided by Lotte Advanced Materials. |