MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Lotte Advanced Materials LOTTMER® SE-064AN TPE
Categories: Polymer; Thermoplastic; Elastomer, TPE

Material Notes: SE-064AN is a SEBS base thermoplastic elastomer(TPE) product. SEBS based TPEs don’t need cross-linking process and can be processed by general thermoplastic processing equipment. It has low compression set, weatherability, cold-resistance and ozone resistance.

Applications: Grip, Gasket etc.

Information provided by Lotte Advanced Materials.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.00 g/ccISO 1183
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 64.0ISO 868
Tensile Strength at Break 7.40 MPaISO 37
Elongation at Break 750 %ISO 37
100% Modulus 1.80 MPaISO 37
Izod Impact, Notched NB
@Temperature -40.0 °C
ISO 180
Tear Strength 25.0 kg(f)/cmASTM D624
 
Processing PropertiesOriginal ValueComments
Processing Temperature 160 - 200 °C
Drying Temperature 80.0 °C
@Time 7200 sec

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PLOTT9206 / 325688

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.