MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

SABIC SABIC® PP 95610CSU10 PP (Global)
Categories: Polymer; Thermoplastic; Polypropylene (PP)

Material Notes: SABIC® PPcompound 95610CSU10 is a mineral filled modified polypropylene. SABIC® PPcompound 95610CSU10 is a material with a high impact and stiffness. The material is part of the SABIC® PP CS systems ans also available as a CS system: using a mixture of 80% SABIC® PP 95610 and 20% SABIC® PPcompound 20MBTFU yields similar properties as listed below. SABIC®PPcompound 95610CSU10 is a designated automotive grade. IMDS ID: 16485548

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.961 g/cc0.0347 lb/in³Injection molded sample ISO527-1A; ISO 1183
Filler Content 10 %10 %SABIC method
Linear Mold Shrinkage 0.012 cm/cm0.012 in/inInjection molded plaque 65x65x3.2mm; SABIC method
Melt Flow 5.4 g/10 min
@Load 2.16 kg,
Temperature 230 °C
5.4 g/10 min
@Load 4.76 lb,
Temperature 446 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 5959ISO 868
Tensile Strength at Break 19.0 MPa2760 psiISO 527/1A
Tensile Strength, Yield 17.0 MPa2470 psiISO 527/1A
Elongation at Break 700 %700 %ISO 527/1A
Tensile Modulus 1.05 GPa152 ksiISO 527/1A
Flexural Modulus 1.10 GPa160 ksiISO 178/1A
Izod Impact, Notched (ISO) NBNBISO 180/1A
 10.0 kJ/m²
@Temperature -20.0 °C
4.76 ft-lb/in²
@Temperature -4.00 °F
N.B.: No Break; ISO 180/1A
 NB
@Temperature 0.000 °C
NB
@Temperature 32.0 °F
ISO 180/1A
Charpy Impact Unnotched NBNBISO 179/1eU
Charpy Impact, Notched NBNBISO 179/1eA
 
Thermal PropertiesMetricEnglishComments
CTE, linear 110 µm/m-°C
@Temperature 23.0 - 80.0 °C
61.1 µin/in-°F
@Temperature 73.4 - 176 °F
ASTM D696
Deflection Temperature at 0.46 MPa (66 psi) 80.0 °C176 °FISO 75
Vicat Softening Point 120 °C248 °Fat 10 N (VST/A); ISO 306/A

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PSABI11512 / 244979

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.