MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
SABIC SABIC® PP 95610CSU10 PP (Global)
Categories: Polymer; Thermoplastic; Polypropylene (PP)

Material Notes: SABIC® PPcompound 95610CSU10 is a mineral filled modified polypropylene. SABIC® PPcompound 95610CSU10 is a material with a high impact and stiffness. The material is part of the SABIC® PP CS systems ans also available as a CS system: using a mixture of 80% SABIC® PP 95610 and 20% SABIC® PPcompound 20MBTFU yields similar properties as listed below. SABIC®PPcompound 95610CSU10 is a designated automotive grade. IMDS ID: 16485548

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.961 g/ccInjection molded sample ISO527-1A; ISO 1183
Filler Content 10 %SABIC method
Linear Mold Shrinkage 0.012 cm/cmInjection molded plaque 65x65x3.2mm; SABIC method
Melt Flow 5.4 g/10 min
@Load 2.16 kg,
Temperature 230 °C
ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 59ISO 868
Tensile Strength at Break 19.0 MPaISO 527/1A
Tensile Strength, Yield 17.0 MPaISO 527/1A
Elongation at Break 700 %ISO 527/1A
Tensile Modulus 1050 MPaISO 527/1A
Flexural Modulus 1100 MPaISO 178/1A
Izod Impact, Notched (ISO) NBISO 180/1A
 10.0 kJ/m²
@Temperature -20.0 °C
N.B.: No Break; ISO 180/1A
 NB
@Temperature 0.000 °C
ISO 180/1A
Charpy Impact Unnotched NBISO 179/1eU
Charpy Impact, Notched NBISO 179/1eA
 
Thermal PropertiesOriginal ValueComments
CTE, linear 110 µm/m-°C
@Temperature 23.0 - 80.0 °C
ASTM D696
Deflection Temperature at 0.46 MPa (66 psi) 80.0 °CISO 75
Vicat Softening Point 120 °Cat 10 N (VST/A); ISO 306/A

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSABI11512 / 244979

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.