MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

3M 8403 Polyester Tape
Categories: Polymer; Tape

Material Notes: 3M™ Polyester Tape 8403 has a silicone adhesive for composite bonding and splicing of many silicone coated papers and films.

Information provided by 3M

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Thickness 35.6 microns1.40 milBacking; ASTM D3752
 61.0 microns2.40 milTotal; ASTM D3752
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 134.3 MPa19480 psiASTM D3759
Elongation at Break 150 %150 %ASTM D3759
Peel Strength 0.29582 kN/m1.6875 pliAdhesion to Steel; ASTM D3330
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 177 °C351 °F
 
Descriptive Properties
Adhesive TypeSilicone
AppearanceTranslucent green

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Uranium, U; Cast
Teknor Apex ELEXAR® EL 8421 Thermoplastic Elastomer
Plutonium, Pu
Overview of materials for Polyethylene Terephthalate (PET), Unreinforced
Overview of materials for Polyethylene Terephthalate (PET), Glass Fiber Filled, Flame Retardant

PMM34503 / 169250

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.