MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Plutonium, Pu
Categories: Metal; Nonferrous Metal; Pure Element

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 19.0 g/cc0.686 lb/in³
 
Chemical PropertiesMetricEnglishComments
Atomic Mass 244244Longest-Lived Isotope (1995)
Atomic Number 9494
X-ray Absorption Edge 0.10228 Å0.10228 ÅK
 0.53662 Å0.53662 ÅLI
 0.55712 Å0.55712 ÅLII
 0.68637 Å0.68637 ÅLIII
Electronegativity 1.31.3Pauling
Ionic Radius 0.930 Å0.930 ÅCrystal Ionic Radius for Valence +4
 1.08 Å1.08 ÅCrystal Ionic Radius for Valence +3
Electrochemical Equivalent 2.8 g/A/h2.8 g/A/h
 
Mechanical PropertiesMetricEnglishComments
Hardness, Brinell 242242Converted from Vickers for 3000 kg load/10 mm ball Brinell test.
Hardness, Rockwell A 6262Converted from Vickers.
Hardness, Rockwell C 2222Converted from Vickers.
Hardness, Vickers 250250
Tensile Strength, Ultimate 400 MPa58000 psiCast Alpha
Tensile Strength, Yield 275 MPa39900 psiCast Alpha
Elongation at Break 0.20 - 0.50 %0.20 - 0.50 %Cast Alpha
Modulus of Elasticity 96.5 GPa14000 ksiCast
Compressive Yield Strength 415 MPa60200 psi
Ultimate Compressive Strength 830 MPa120000 psi
Poissons Ratio 0.15 - 0.210.15 - 0.21
Fatigue Strength 90.0 MPa
@# of Cycles 1.00e+8
13100 psi
@# of Cycles 1.00e+8
rotating beam
Shear Modulus 45.0 GPa6530 ksi
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.000150 ohm-cm0.000150 ohm-cm
Magnetic Susceptibility 0.00000220.0000022cgs/g
 
Thermal PropertiesMetricEnglishComments
Heat of Fusion 13.0 J/g5.59 BTU/lb
CTE, linear  35.0 µm/m-°C
@Temperature 250 °C
19.4 µin/in-°F
@Temperature 482 °F
bulk gamma phase
 37.0 µm/m-°C
@Temperature 500 °C
20.6 µin/in-°F
@Temperature 932 °F
bulk gamma phase
 55.0 µm/m-°C
@Temperature 20.0 - 100 °C
30.6 µin/in-°F
@Temperature 68.0 - 212 °F
Thermal Conductivity 8.40 W/m-K58.3 BTU-in/hr-ft²-°F
Melting Point 640 °C1180 °F
Boiling Point 3228 °C5842 °F
 
Component Elements PropertiesMetricEnglishComments
Plutonium, Pu 100 %100 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Silver, Ag
Uranium, U; Cast
Aluminum, Al
Carbon-Core CarbonFoam PU 2 R PU
Americium, Am

AMEPu00 / 88

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.