PlasGlas 40118 is a specially formulated glass-filled polyester bulk molding compound intended for use as a floor tile material. As such, it has superior flammability ratings, low smoke generation, and excellent smoke toxicity ratings. It is offered in bulk or extruded form, and is currently available in natural. Other colors available upon request. Data provided by Plaslok Corporation. Plaslok Corporation was purchased by Plastics Engineering Company in March 2000. The Plaslok name is no longer used on any products. |