MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Orion Engineered Carbons PUREX® HS 45-RP Carbon Black
Categories: Carbon; Carbon Black

Material Notes: Carbon black grade for manufacture of mechanical rubber goods such as extruded profiles and seals

Information provided by Orion Engineered Carbons.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Bulk Density 0.365 g/cc0.0132 lb/in³Pour Density; ASTM D 1513
Oil Absorption 85 %85 %(ml/100 g); Compressed Sample; ASTM D 3493
 121 %121 %(ml/100 g); ASTM D 2414
Loss On Ignition <= 0.50 %<= 0.50 %Heating Loss; ASTM D 1509
Specific Surface Area 39 m²/g39 m²/gStatistical thickness surface area; ASTM D 6556
Iodine Absorption Number 4343mg/g; ASTM D 1510
 
Descriptive Properties
Fines< 7.0 %ASTM D 1508
Individual Pellet Hardness< 40 gASTM D 5230, average 1.4 - 1.7 mm
Sieve Residue< 50 ppmASTM D 1514

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Graphite, Carbon, C
AISI 1045 Steel, Quenched and Tempered to 390 HB
Aremco Graphi-Bond™ 551-R
Aremco Graphi-Bond™ 551-RN High Temperature Ceramic Adhesive/Paste, Graphite Filled
Aremco Graphi-Bond™ 669 High Temperature Ceramic Adhesive/Paste, Graphite Filled

EORION932 / 159756

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.