MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Aremco

Aremco Graphi-Bond™ 551-RN High Temperature Ceramic Adhesive/Paste, Graphite Filled
Categories: Carbon; Graphite

Material Notes: Aremco’s high temperature graphite adhesives are formulated using both phenolic and silicate binders to bond carbon, carbon fiber composite (CFC), and graphite components, structures and tools used in a broad range of applications to 5400°F (2985°C).

Typical Applications:
Bonding

  • Graphite Insulation
  • Carbon Brick
  • Carbon Foam & Felt
  • Carbon Fiber Composites
  • Graphite Rams & Punches
  • Graphite Sight Tubes
  • Graphite Pour Spouts
  • Graphite Foil to Rigid Graphite Insulation
  • Graphite Foil to CFC
Laminating
  • Carbon Fiber Composites
Reparing
  • Graphite Trays, Dies, Jigs, Fixtures
  • Patch Holes
  • Fix Scratches
  • Repair Susceptors
Sealing
  • Porosity in Carbon & Graphite

Vendors: Aremco’s ceramic and graphite adhesives are ideal for bonding, potting and sealing probes, sensors, halogen lamps, igniters, power resistors, cartridge heaters, filters, fiberoptics, honeycombs, and graphite structures to 3200°F (1760°C). Visit us today at Aremco.com or call 1 (845) 268-0039 to speak with an engineer.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 1.45 - 1.50 g/cc0.0524 - 0.0542 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Shear Strength 5.58 MPa810 psiLap, RT Post-Cure
 
Electrical PropertiesMetricEnglishComments
Dielectric Strength 2.95 kV/mm75.0 kV/in
 
Thermal PropertiesMetricEnglishComments
CTE, linear 7.38 µm/m-°C4.10 µin/in-°F
Maximum Service Temperature, Inert 2980 °C5400 °F
 
Processing PropertiesMetricEnglishComments
Processing Temperature 4.44 - 32.2 °C40.0 - 90.0 °FApplication Temperature
Cure Time  120 min
@Temperature 129 °C
2.00 hour
@Temperature 265 °F
Step 1, preceded by 1-4 hour air set
 120 min
@Temperature 260 °C
2.00 hour
@Temperature 500 °F
Step 2
Shelf Life 6.00 Month
@Temperature -1.11 - 23.9 °C
6.00 Month
@Temperature 30.0 - 75.0 °F
 
Descriptive Properties
Acid ResistanceGoodafter curing at 700°F for 2 hours
Alkali ResistanceGoodafter curing at 700°F for 2 hours
Bond Type99% Carbonaceous
ColorBlack
Moisture ResistanceExcellentafter curing at 700°F for 2 hours
ThinnerEthanol
ViscosityPaste

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Aremco Graphi-Bond™ 669 High Temperature Ceramic Adhesive/Paste, Graphite Filled
Aremco Pyro-Paint™ 634-CA High Temperature Refractory Coating
Aremco Pyro-Paint™ 634-GR High Temperature Refractory Coating, GR >95%
Aremco Graphi-Bond™ 551-R
Graphite, Carbon, C

CAREM23 / 564

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.