System Message
Advertise with MatWeb!
Data sheets for over
180,000
metals, plastics, ceramics, and composites.
HOME
•
SEARCH
•
TOOLS
•
SUPPLIERS
•
FOLDERS
•
ABOUT US
•
FAQ
•
LOG IN
Recently Viewed Materials (most recent at top)
Login
to see your most recently viewed materials here.
Or if you don't have an account with us yet, then
click here to register.
Searches:
Advanced
|
Category
|
Property
|
Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
(Viewing data as-entered.
Click here
to return)
Lubrizol LifeSciences Pellethane® 5855-70D TPU
Categories:
Polymer
;
Thermoplastic
;
Polyurethane, TP
;
Thermoplastic Polyurethane, Elastomer, Polyester Grade
Material Notes:
Aromatic Polyester-based Thermoplastic Polyurethane (TPU)
Features: High stiffness TPU alloy
Process: Extrusion and Injection Molding.
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Original Value
Comments
Specific Gravity
1.15
g/cc
ASTM D792
Mechanical Properties
Original Value
Comments
Hardness, Shore D
70
ASTM D2240
Tensile Strength, Ultimate
4200
psi
ASTM D412
Elongation at Break
160 %
ASTM D412
100% Modulus
28.3
MPa
@Strain 100 %
ASTM D412
Graves Tear Strength
1100
pli
die C; ASTM D624
Taber Abrasion, mg/1000 Cycles
47
@Load 1.00 kg
H-18; ASTM D3389
Thermal Properties
Original Value
Comments
Melting Point
106
°C
Glass Transition Temp, Tg
-11.0
°C
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to go back to viewing the property data in MatWeb's normal format.
Users viewing this material also viewed the following:
Lubrizol Estane® S375D Thermoplastic Polyurethane
Lubrizol LifeSciences Tecoflex® EG-72D TPU - Clear
Lubrizol LifeSciences Pellethane® 2363-65D TPU
Lubrizol LifeSciences Pellethane® 2363-75D TPU
Covestro Desmopan® 9885DU TPU
PLUBR9040 / 203607
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
webmaster@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.