MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Lubrizol LifeSciences Tecoflex® EG-72D TPU - Clear
Categories: Polymer; Thermoplastic; Polyurethane, TP; Thermoplastic Polyurethane, Elastomer, Ether Grade

Material Notes: Medical Grade Aliphatic Polyether-based Thermoplastic Polyurethane (TPU)

Features: offers an inherent ultraviolet (UV) stability that resists yellowing by aging and sterilization, good mechanical properties and can be color-matched

Process: Extrusion and Injection Molding

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.11 g/cc1.11 g/ccASTM D792
Linear Mold Shrinkage 0.0040 - 0.0060 cm/cm0.0040 - 0.0060 in/inASTM D955
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 6767ASTM D2240
Tensile Strength, Ultimate 55.8 MPa8100 psiASTM D412
Elongation at Break 310 %310 %ASTM D412
100% Modulus 23.4 MPa
@Strain 100 %
3400 psi
@Strain 100 %
ASTM D412
200% Modulus 33.1 MPa
@Strain 200 %
4800 psi
@Strain 200 %
ASTM D412
300% Modulus 49.0 MPa
@Strain 300 %
7100 psi
@Strain 300 %
ASTM D412
Flexural Modulus 0.634 GPa92.0 ksiASTM D790
 
Processing PropertiesMetricEnglishComments
Rear Barrel Temperature 190.5 °C374.9 °FInjection
Front Barrel Temperature 210 °C410 °FInjection
Nozzle Temperature 510 °C950 °FInjection
Zone 1 187.7 °C369.9 °FExtrusion
Zone 2 193.3 °C379.9 °FExtrusion
Zone 3 198.8 °C389.8 °FExtrusion
Zone 4 204.4 °C399.9 °FExtrusion
Adapter Temperature 210 °C410 °FExtrusion
Die Temperature 210 °C410 °FExtrusion
Melt Temperature <= 226.6 °C<= 439.9 °FInjection
Mold Temperature 10.0 - 54.4 °C50.0 - 130 °FInjection

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Lubrizol LifeSciences Tecoflex® EG-68D TPU - Clear
Lubrizol LifeSciences Tecoflex® EG-65D TPU - Clear
Lubrizol LifeSciences Tecoflex® EG-60D TPU - Clear
Lubrizol LifeSciences Tecoflex® EG-80A TPU - Clear
Lubrizol LifeSciences Tecoflex® EG-93A TPU - Clear

PLUBR9052 / 203619

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.