MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
M Chemical GUARD DOG™ UV944 HALS Light Stabilizer
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: GUARD DOG™ UV944 hindered amine light stabilizer is a highly effective radical scavenger that protects polymers against degradation caused by exposure to UV radiation. It is an oligomeric HALS characterized by extremely low volatility, high thermal stability and excellent compatibility with many substrates. its oligomeric structure makes it particularly effective when used in thin section articles such as fiber and film and also finds application as an antioxidant for long term thermal stability and as a heat stabilizer in a wide range of polymers.
Warning: GUARD DOG™ UV944 can adversely react with compounds such as flame retardants, pesticides and fine chemicals that contain sulfur or halogens.

Applications: Extremely effective in LDPE, HDPE, PP resin, elastomers, blends and fiber, XPE, EVA films, ABS, PS, polyurethanes, polyamides and polyacetals and is recommended for thin and thick sections and also in film applications.

Typical Properties:

  • Product Form - Pale yellow powder or pastille
  • Solubility@ 20°C (g/100ml solvent): Acetone - 50, Water - <0.001, Hexane - 40, Methanol - 30, Methyl Chloride - 50, Chloroform - 50, Benzene - 50

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.01 g/cc
@Temperature 20.0 °C
Volatiles <= 1.0 %
Molecular Weight 2000 - 3100 g/mol
Ash <= 0.10 %
 
Thermal PropertiesOriginal ValueComments
Melting Point 100 - 135 °C
Flash Point >= 160 °C
 
Optical PropertiesOriginal ValueComments
UV Transmittance >= 93 %
@Thickness 0.425 mm
 >= 95 %
@Thickness 0.450 mm
 
Component Elements PropertiesOriginal ValueComments
Nitrogen, N 4.6 %
 
Descriptive Properties
CAS Number70624-18-9 (USA) / 71878-19-8
Molecular Formula(C35H54N8)nn = 4-5
NamePoly-{[6-[(1,1,3,3-tetramethylbutyl)amino]-1,3,5-triazine-2,4-diyl][(2,2,6,6-tetramethyl-4-piperidinyl)imino] 1-1,6-hexanediyl[(2,2,6,6-tetramethyl-4-piperdinyl)imino]}
Recommended Dosage0.10 - 0.30%depending upon the substrate and performance requirements

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
M Chemical GUARD DOG™ UV234 Light Absorber, Benzotriazole Derivative
M Chemical GUARD DOG™ UV360 Light Absorber
M Chemical GUARD DOG™ UV531 Light Absorber (Flake or Powder), Benzophenone Derivative
Global EPP PA 6C OFN Cast Polyamide 6 + Blended Liquid Lubricant
Global EPP PA 6C MOLY Cast Polyamide 6 + MoS2

PMCHEM915 / 135154

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.