Desmoderm® KB2H Granular is a one-component polyester urethane based on an aromatic diisocyanate. Uses: Desmoderm® KB2H is used as the hard component in the polyurethane coagulation process. Desmoderm® KB2H Granular is suitable for use in the manufacture of materials for shoe uppers, shoe linings and bags/luggage. Information provided by Covestro |