MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Covestro Desmoderm® KB2H Granular Polyurethane
Categories: Polymer; Thermoplastic; Polyurethane, TP

Material Notes: Desmoderm® KB2H Granular is a one-component polyester urethane based on an aromatic diisocyanate.

Uses: Desmoderm® KB2H is used as the hard component in the polyurethane coagulation process. Desmoderm® KB2H Granular is suitable for use in the manufacture of materials for shoe uppers, shoe linings and bags/luggage.

Information provided by Covestro

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Viscosity 4000 - 20000 cP4000 - 20000 cPUntempered, (20 % in dimethylformamide); DIN EN ISO 3219/A.3
 4000 - 60000 cP4000 - 60000 cPTempered, 5 h, 120°C, (20% in dimethylformamide); DIN EN ISO 3219/A.3
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 40.0 - 50.0 MPa5800 - 7250 psiDIN 53504
 30.0 - 40.0 MPa
@Temperature 70.0 °C
4350 - 5800 psi
@Temperature 158 °F
after 14 d hydrolysis (95 % rel. humidity); DIN 53504
Elongation at Break 200 - 300 %200 - 300 %DIN 53504
100% Modulus 20.0 - 25.0 MPa
@Strain 100 %
2900 - 3630 psi
@Strain 100 %
DIN 53504
 
Thermal PropertiesMetricEnglishComments
Softening Point 180 - 190 °C356 - 374 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Covestro Desmopan® 1045D TPU
Covestro DUREFLEX® U073 TPU
Covestro Desmopan® 453 DPS 041 TPU
Covestro Desmopan® 3055D - DPS066 TPU
Covestro Desmopan® 1092A TPU

PCOVEST0297 / 202080

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.