MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Refractory Metals

Plansee WL-S Lanthanum Oxide-doped Tungsten
Categories: Metal; Metal Matrix Composite; Nonferrous Metal; Refractory Metal; Tungsten Alloy

Material Notes: Tungsten alloy suitable for use as support rods in high-pressure discharge lamps.

Characteristics (compared to other tungsten-lanthanum oxide alloys):

  • More fine-grained microstructure
  • Higher strength at high thermal loads

Information provided by Plansee.

Vendors: PLANSEE SE: Whether it's high temperatures, aggressive chemicals or extreme mechanical loading: PLANSEE supplies a suitable product solution in refractory metals or composite materials. As the world market leader in powder metallurgically produced high performance materials we combine outstanding materials knowledge with profound applications and technology know-how. Visit us at www.plansee.com.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density >= 18.75 g/cc>= 0.6774 lb/inĀ³
 
Component Elements PropertiesMetricEnglishComments
Other, each 1.0 %1.0 %Lanthanum Oxide
Tungsten, W 99 %99 %
 
Descriptive Properties
Creep Resistancemuch greater than pure W
Ductilitygreater than pure W
Fineness of Grainmuch greater than pure W
Machinability/Workabilitymuch greater than pure W
Recrystallization Temperaturemuch greater than pure W
Stability at High Temperaturemuch greater than pure W

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Plansee W-20Cu Tungsten-Copper Composite
Plansee W-15Cu Tungsten-Copper Composite
Plansee W-10Cu Tungsten-Copper Composite
Plansee WCu22 WCu (80:20)
Plansee WCu20 WCuNi

NPLAM928 / 135484

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.