MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Refractory Metals

Plansee WCu22 WCu (80:20)
Categories: Metal; Metal Matrix Composite; Nonferrous Metal; Tungsten Alloy

Material Notes:

Information provided by Plansee.

Key Words: Tungsten Copper
Vendors: PLANSEE SE: Whether it's high temperatures, aggressive chemicals or extreme mechanical loading: PLANSEE supplies a suitable product solution in refractory metals or composite materials. As the world market leader in powder metallurgically produced high performance materials we combine outstanding materials knowledge with profound applications and technology know-how. Visit us at www.plansee.com.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 15.25 g/cc0.5509 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Vickers 200200HV10
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.00000500 ohm-cm0.00000500 ohm-cm
 
Thermal PropertiesMetricEnglishComments
CTE, linear 8.70 µm/m-°C4.83 µin/in-°F
Thermal Conductivity 200 W/m-K
@Temperature 20.0 °C
1390 BTU-in/hr-ft²-°F
@Temperature 68.0 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Plansee W-10Cu Tungsten-Copper Composite
H.C. Starck WCu 80/20 Tungsten-Copper Composite Material
H.C. Starck WCu 70/30 Tungsten-Copper Composite Material
Plansee W-20Cu Tungsten-Copper Composite
Plansee WCu20 WCuNi

NPLAM935g / 185682

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.