MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
A. Schulman Alcryn® 4070 NC Melt-Processible Rubber  (discontinued **)
Categories: Polymer; Thermoplastic; Elastomer, TPE; Thermoplastic Elastomer, Melt-Processible Rubber

Material Notes: Alcryn® is a true thermoplastic elastomer, based on a partially cross-linked, chlorinated olefin interpolymer alloy. It is designed for the manufacture of rubber parts with high productivity on thermoplastic processing equipment. 4000 series characteristics: moderate flow in general plastics processing; not recommended for injection molding; excellent for complex extrusions; black grades have excellent weather resistance.

Former product line of Advanced Polymer Alloys (APA), acquired by A. Schulman in 2014.

Key Words: Chlorinated Olefin Interpolymer Alloy; Advanced Polymer Alloys; Thermoplastic Elastomer (TPE)
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.25 g/ccASTM D471
Viscosity 500000 cP
@Shear Rate 300 1/s,
Temperature 190 °C
ASTM D3835
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 70ASTM D2240
Tensile Strength, Yield 8.80 MPaASTM D412
Elongation at Break 440 %ASTM D412
Tensile Modulus 0.00390 GPaASTM D412
Shear Modulus 0.00240 GPaASTM D1043
Graves Tear Strength 39.0 kN/m(Die C); ASTM D624
Taber Abrasion, mg/1000 Cycles 4.0CS-17 Wheel, 1000g load; ASTM D3389
Compression Set 74 %
@Temperature 100 °C
22 hr at 100°C; ASTM D395
 21 %
@Temperature 24.0 °C,
Time 79200 sec
ASTM D395
 
Thermal PropertiesOriginal ValueComments
Brittleness Temperature -60.0 °CASTM D746
Clash Berg Stiffness Temperature -20.0 °C69 MPa; ASTM D1043
 
Processing PropertiesOriginal ValueComments
Processing Temperature 166 °CASTM D3835

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
A. Schulman DuraGrip™ 6070 BK Thermoplastic Elastomer
Ineos Nova Zylar® 631 Clear Impact Modified Acrylic Copolymer
Entec Hylex® P1310FR Polycarbonate
Braskem TR3350CW2 Polypropylene Random Copolymer

PRAP15 / 65272

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.