MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

A. Schulman DuraGrip™ 6070 BK Thermoplastic Elastomer
Categories: Polymer; Thermoplastic; Elastomer, TPE

Material Notes: DuraGrip® DGR 6070NC is designed to be a general purpose Thermoplastic Elastomer (TPE) that is easy to use in the injection molding process. DGR 6070NC has an excellent soft touch feel, will bond to olefinics, is easy to color, and is available in FDA compliant formulations. DuraGrip® is not hygroscopic and under normal conditions does not require drying.

Information provided by Advanced Polymer Alloys

Former product line of Advanced Polymer Alloys (APA), acquired by A. Schulman in 2014.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 0.985 g/cc0.985 g/ccASTM D471
Viscosity 130000 cP
@Shear Rate 300 1/s,
Temperature 190 °C
130000 cP
@Shear Rate 300 1/s,
Temperature 374 °F
ASTM D3835
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 72725 Sec; ASTM D2240
Tensile Strength at Break 8.34 MPa1210 psiASTM D412
Elongation at Break 640 %640 %ASTM D412
100% Modulus 2.62 MPa
@Strain 100 %
380 psi
@Strain 100 %
ASTM D412
300% Modulus 3.43 MPa
@Strain 300 %
497 psi
@Strain 300 %
ASTM D412
Graves Tear Strength 28.6 kN/m
@Temperature 24.0 °C
163 pli
@Temperature 75.2 °F
Die C; ASTM D624
 
Processing PropertiesMetricEnglishComments
Melt Temperature 180 - 230 °C356 - 446 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Dow LDPE 955I Low Density Polyethylene
A. Schulman Alcryn® 4070 NC Melt-Processible Rubber
Teknor Apex Medalist® MD-160 Thermoplastic Elastomer
Ineos Nova Zylar® 631 Clear Impact Modified Acrylic Copolymer
ExxonMobil Santoprene® 281-87MED Thermoplastic Elastomer

PAPA054 / 24121

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.