MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Barlog Plastics KEBAPEAK XC1730 PEEK; 30% carbon fiber reinforced
Categories: Polymer; Thermoplastic; Polyketone; Polyetheretherketone (PEEK); Polyetheretherketone, PEEK, Carbon Fiber Filled

Material Notes: PEEK-CF30

Information provided by BARLOG plastics GmbH.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.40 g/cc0.0506 lb/in³ISO 1183
Water Absorption 0.040 %0.040 %similar to ISO 62 test
Linear Mold Shrinkage, Flow 0.0020 cm/cm0.0020 in/inISO 294-4
Linear Mold Shrinkage, Transverse 0.0060 cm/cm0.0060 in/inISO 294-4
 
Mechanical PropertiesMetricEnglishComments
Tensile Modulus 23.5 GPa3410 ksiISO 527-1
Charpy Impact Unnotched 4.50 J/cm²21.4 ft-lb/in²ISO 179-1eU
Charpy Impact, Notched 0.650 J/cm²3.09 ft-lb/in²ISO 179-1eA
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1000 ohm-cm1000 ohm-cmIEC 60093
 
Thermal PropertiesMetricEnglishComments
Melting Point 343 °C649 °F10°C/min; ISO 11357-1/-3
Deflection Temperature at 1.8 MPa (264 psi) 310 °C590 °FISO 75-1/-2
Flammability, UL94 V-0
@Thickness 0.800 mm
V-0
@Thickness 0.0315 in
IEC 60695-11-10
 
Descriptive Properties
Resin TypePEEK-CF30

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Akro-Plastic Akrotek® PEEK CF 30 black (5049) PEEK, Dry, 30% Carbon Filled
Evonik VESTAKEEP® 2000 CF30 PEEK
Overview of materials for Polyetheretherketone, Unreinforced
LATI Larpeek 10 K/40 PEEK, 40% Carbon Fiber Reinforced
LATI Larpeek 50 K/30 PEEK, 30% Carbon Fiber Reinforced

PBARLO920 / 149938

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.