MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Evonik ROHACELL® 110 RIST-HT Polymethacrylimide Foam
Categories: Polymer; Thermoset; Polymethacrylimide

Material Notes: ROHACELL® RIST is a closed-cell rigid foam based on polymethacrylimide (PMI) chemistry, which does not contain any CFC's. We have specially developed ROHACELL® RIST for use as a structural core in connection with vacuum infusion processes. Its mechanical and thermo-mechanical properties are similar to those of ROHACELL® WF. Its cell size, however, represents an optimal compromise between low resin uptake—about 50% less than for ROHACELL® WF—and satisfactory bonding of the facings to the foam core. Its optimized cell structure makes ROHACELL® RIST particularly suitable for vacuum infusion and RTM processes, where it can be used at temperatures of 130°C and up to a pressure of 0.7 MPa. Heat treated ROHACELL® RIST-HT allows safe and stable processing at a temperature of 180°C with pressures of up to 0.7 MPa.

Information provided by Evonik

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.110 g/ccISO 845
Water Absorption <= 0.50 %
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 3.70 MPaISO 527-2
Elongation at Break 3.0 %ISO 527-2
Modulus of Elasticity 0.180 GPaISO 527-2
Compressive Strength 3.60 MPaISO 844
Poissons Ratio 0.29Calculated
Shear Modulus 0.0700 GPaASTM C273
Shear Strength 2.40 MPaASTM C273
 
Thermal PropertiesOriginal ValueComments
CTE, linear 34.3 µm/m-°C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Evonik Rohacell® 110 A Aircraft Grade Polymethacrylimide (PMI) Foam
Evonik Rohacell® 51 FX Polymethacrylimide (PMI) Rigid Foam Plastic
Evonik Rohacell® 71 S Self-Extinguishing Grade Polymethacrylimide (PMI) Foam
ZEON Hydrin® C2000 Polyepichlorohydrin Elastomer
Evonik ROHACELL® 110 SL Polymethacrylimide Foam

PEVONIL316 / 196520

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.