MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

ZEON Hydrin® C2000 Polyepichlorohydrin Elastomer
Categories: Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE)

Material Notes: Hydrin C2000 is an epichlorohydrin/ethylene oxide copolymer with high oil, fuel and solvent resistance. Compounds using Hydrin C2000 typically exhibit good heat resistance, excellent ozone resistance along with outstanding gas impermeability. Sufficient antioxidant is added during the manufacturing process for normal aging conditions.

Fuel pump diaphragms, hose, coated fabrics and vibration mounts. Can also impart antistatic properties to plastics.

Key Words: ECO
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.28 g/cc1.28 g/cc
Mooney Viscosity 90 - 102
@Temperature 100 °C
90 - 102
@Temperature 212 °F
(1+4)
Ash <= 1.0 %<= 1.0 %Zeon Test #1358
 
Thermal PropertiesMetricEnglishComments
Glass Transition Temp, Tg -41.0 °C-41.8 °F
 
Component Elements PropertiesMetricEnglishComments
Chlorine, Cl 24.5 - 26.5 %24.5 - 26.5 %
H2O, Water <= 1.0 %<= 1.0 %Zeon Test #1361

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
BYK Cloisite® 10A Nanoclay
Cast Stainless Steel CA6NM, ASTM A352
Evonik VESTAGON® B 1065 PUR System
Evonik ROHACELL® 110 RIST-HT Polymethacrylimide Foam
Envalior Durethan® BKV 230 H3.0 000000 Nylon 6-Copolymer, 30% Glass Fibers

PZEONC53 / 73112

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.