MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Rogers Arlon CuClad 6250 Bonding Film
Categories: Polymer; Film; Thermoplastic

Material Notes:
  • Thermoplastic Bonding Films
  • Similar Dk and Df range to many PTFE laminates

Benefits:

  • Can be reheated to remelt and reflow bonding film
  • Excellent Electrical Properties

Typical Applications:

  • Stripline Circuitry
  • Multi-Layer Boards and Hybrid Con instructions for Microwave applications
  • Attachment of Circuit Boards to Heavy Plate Heat Sinks

Information provided by Arlon Materials for Electronics (MED); now a part of Rogers Corporation.

Vendors: Arlon Materials for Electronics (MED) is a major manufacturer of specialty high performance laminate and prepreg materials for use in a wide variety of printed circuit board (PCB) applications and in several distinctive markets.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 0.930 g/cc0.0336 lb/in³ASTM D1505
Thickness 0.0381 microns0.00150 mil
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+16 ohm-cm1.00e+16 ohm-cmASTM D257
Dielectric Constant 2.32
@Frequency 1e+10 Hz
2.32
@Frequency 1e+10 Hz
IPC TM-650
Dielectric Strength >= 39.4 kV/mm>= 1000 kV/inASTM D149
Dissipation Factor 0.0013
@Frequency 1e+10 Hz
0.0013
@Frequency 1e+10 Hz
IPC TM-650
Arc Resistance 130 - 140 sec130 - 140 secASTM D495
 
Thermal PropertiesMetricEnglishComments
Thermal Conductivity 0.170 W/m-K1.18 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air <= 75.0 °C<= 167 °FContinuous Use
Brittleness Temperature -60.0 °C-76.0 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Parker Chomerics CHO-SHIELD® 4994 Conductive Flexible Coating
DuPont Teijin Films Mylar® C Polyester Film, 10 Gauge
Dow FOX® PMCP13 Flowable Oxide
Titanium Nitride (TiN) Coating
Rogers Arlon CLTE-P Pre-Preg Bonding Layer

PARLM9897 / 149050

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.