MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Rogers Arlon CLTE-P Pre-Preg Bonding Layer
Categories: Polymer; Thermoplastic; Fluoropolymer; Polytetrafluoroethylene (PTFE)

Material Notes: Arlon's CLTE-P Prepreg Bonding Layer is a ceramic filled PTFE coated glass stock that is used as a bonding ply for CLTE, CLTE-X or CLTE-AT laminates. CLTE-P is a pre-preg material that consists of woven fiberglass fabric coated with a proprietary resin formulation. The Proprietary resin is thermoplastic, not thermoset in nature.

Information provided by Arlon Materials for Electronics (MED); now a part of Rogers Corporation.

Vendors: Arlon Materials for Electronics (MED) is a major manufacturer of specialty high performance laminate and prepreg materials for use in a wide variety of printed circuit board (PCB) applications and in several distinctive markets.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 2.38 g/cc0.0860 lb/in³ASTM D792 Method A
Water Absorption 0.040 %0.040 %IPC TM-650 2.6.2.2
Thickness 0.0610 microns0.00240 milAfter lamination
 0.0813 microns0.00320 milAs received
 1.57 microns0.0620 milThickness of laminate tested
Outgassing - Total Mass Loss  0.00 %
@Pressure <=1.33e-10 MPa,
Temperature 125 °C
0.00 %
@Pressure <=1.93e-8 psi,
Temperature 257 °F
Water Vapor Recovered; NASA SP-R-0022A
 0.020 %
@Pressure <=1.33e-10 MPa,
Temperature 125 °C
0.020 %
@Pressure <=1.93e-8 psi,
Temperature 257 °F
NASA SP-R-0022A
Collected Volatile Condensable Material 0.00 %
@Pressure <=1.33e-10 MPa,
Temperature 125 °C
0.00 %
@Pressure <=1.93e-8 psi,
Temperature 257 °F
NASA SP-R-0022A
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 48.3 MPa7000 psiCross; ASTM D882
 56.5 MPa8200 psiMachine; ASTM D882
Modulus of Elasticity 3.19 GPa462 ksiCross; ASTM D638
 3.25 GPa471 ksiMachine; ASTM D638
Flexural Modulus >= 2.59 GPa>= 375 ksiASTM D790
Compressive Modulus 1.55 GPa225 ksiASTM D695
Peel Strength 1.23 kN/m7.00 pliAfter Thermal Stress; IPC TM-650 2.4.8
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.40e+14 ohm-cm1.40e+14 ohm-cmC96/35/90; IPC TM-650 2.5.17.1
Surface Resistance 1.30e+12 ohm1.30e+12 ohmC96/35/90; IPC TM-650 2.5.17.1
Dielectric Constant 2.94
@Frequency 1e+10 Hz
2.94
@Frequency 1e+10 Hz
C23/50; IPC TM-650 2.5.5.5
Dielectric Breakdown >= 45000 V>= 45000 VD48/50; ASTM D149
Dissipation Factor 0.0025
@Frequency 1e+10 Hz
0.0025
@Frequency 1e+10 Hz
C23/50; IPC TM-650 2.5.5.5
Arc Resistance >= 180 sec>= 180 secD48/50; ASTM D495
 
Thermal PropertiesMetricEnglishComments
CTE, linear  10.0 µm/m-°C
@Temperature 0.000 - 100 °C
5.56 µin/in-°F
@Temperature 32.0 - 212 °F
x direction; IPC TM-650 2.4.24
 12.0 µm/m-°C
@Temperature 0.000 - 100 °C
6.67 µin/in-°F
@Temperature 32.0 - 212 °F
y direction; IPC TM-650 2.4.24
CTE, linear, Transverse to Flow 35.0 µm/m-°C
@Temperature 0.000 - 100 °C
19.4 µin/in-°F
@Temperature 32.0 - 212 °F
z direction; IPC TM-650 2.4.24
Thermal Conductivity 0.500 W/m-K
@Temperature 100 °C
3.47 BTU-in/hr-ft²-°F
@Temperature 212 °F
ASTM E1225
Flammability, UL94 V-0V-0Vertical Burn
 
Descriptive Properties
Temperature Coefficient of Dielectric (ppm/°C)-12IPC TM-650 2.5.5.5 (-10 - 140°C)

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Rogers Corporation 3001 Thermoplastic Chloro-Fluorocopolymer Bonding Film
Rogers Arlon CuClad 6700 Bonding Film
Rogers Arlon CuClad 6250 Bonding Film
Honeywell UltRx 400 CTFE Homopolymer, Barrier Film
Honeywell ACLAR® UltRx 3000 CTFE Homopolymer, Barrier Film

PARLM9895 / 149048

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.