MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Borealis CG9620 High Density Polyethylene
Categories: Polymer; Film; Thermoplastic; Polyethylene (PE); High Density (HDPE); High Density Polyethylene (HDPE), Film Grade

Material Notes: CG9620 is a high density polyethylene film grade which combine excellent extrusion behavior with superior mechanical properties. Applications: CG9620 is recommended for coated film and co-extrusion applications.

Information provided by Borealis AG

Key Words: PE
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.962 g/ccISO 1183
Melt Flow 12 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ISO 1133
Coating Weight 9.00 g/m²BTM 14922
 
Thermal PropertiesOriginal ValueComments
Melting Point 131 °CDSC; ISO 3146
 
Descriptive Properties
Coating Speed (m/min)> 400 m/minBTM 14921

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Borealis Borstar® FB1460 HDPE for Film
Overview of materials for High Density Polyethylene (HDPE), Film Grade
Borealis CA7230 Low Density Polyethylene
Chevron Phillips HiD® 9605D HDPE Cast Film Resin
Chevron Phillips Marlex® 9608XD HDPE Film Grade

PBOREA399 / 108658

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.