MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Overview of materials for High Density Polyethylene (HDPE), Film Grade
Categories: Polymer; Film; Thermoplastic; Polyethylene (PE); High Density (HDPE); High Density Polyethylene (HDPE), Film Grade

Material Notes: This property data is a summary of similar materials in the MatWeb database for the category "High Density Polyethylene (HDPE), Film Grade". Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.917 - 0.968 g/cc0.0331 - 0.0350 lb/in³Average value: 0.951 g/cc Grade Count:209
Moisture Vapor Transmission 0.100 - 0.260 cc-mm/m²-24hr-atm0.254 - 0.660 cc-mil/100 in²-24hr-atmAverage value: 0.172 cc-mm/m²-24hr-atm Grade Count:14
 0.00418 - 2.64 cc-mm/m²-24hr-atm
@Temperature 38.0 - 38.0 °C
0.0106 - 6.71 cc-mil/100 in²-24hr-atm
@Temperature 100 - 100 °F
Average value: 1.32 cc-mm/m²-24hr-atm Grade Count:2
Water Vapor Transmission 0.260 - 62.1 g/m²/day0.0167 - 4.00 g/100 in²/dayAverage value: 8.93 g/m²/day Grade Count:13
 0.500 - 15.5 g/m²/day
@Temperature 37.8 - 38.0 °C
0.0322 - 0.998 g/100 in²/day
@Temperature 100 - 100 °F
Average value: 5.63 g/m²/day Grade Count:18
Oxygen Transmission 1.77 - 138 cc-mm/m²-24hr-atm4.49 - 351 cc-mil/100 in²-24hr-atmAverage value: 64.4 cc-mm/m²-24hr-atm Grade Count:4
Oxygen Transmission Rate 465 - 5580 cc/m²/day29.9 - 359 cc/100 in²/dayAverage value: 2030 cc/m²/day Grade Count:13
Environmental Stress Crack Resistance 2.00 - 1500 hour2.00 - 1500 hourAverage value: 768 hour Grade Count:11
 24.0 - 24.0 hour
@Temperature 50.0 - 50.0 °C
24.0 - 24.0 hour
@Temperature 122 - 122 °F
Average value: 1000 hour Grade Count:6
Oxidative Induction Time (OIT) 40.0 - 55.0 min
@Temperature 200 - 200 °C
40.0 - 55.0 min
@Temperature 392 - 392 °F
Average value: 48.8 min Grade Count:4
Thickness 10.0 - 75.0 microns0.394 - 2.95 milAverage value: 26.8 microns Grade Count:93
Melt Flow 0.0270 - 55.0 g/10 min0.0270 - 55.0 g/10 minAverage value: 5.01 g/10 min Grade Count:210
Base Resin Melt Index 0.0500 - 18.0 g/10 min0.0500 - 18.0 g/10 minAverage value: 4.90 g/10 min Grade Count:4
Ash 0.0300 - 0.0600 %0.0300 - 0.0600 %Average value: 0.0544 % Grade Count:8
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 28.0 - 69.028.0 - 69.0Average value: 61.7 Grade Count:27
Tensile Strength, Ultimate 23.0 - 89.2 MPa3340 - 12900 psiAverage value: 36.4 MPa Grade Count:21
Film Tensile Strength at Yield, MD 11.6 - 51.7 MPa1680 - 7500 psiAverage value: 29.2 MPa Grade Count:94
Film Tensile Strength at Yield, TD 12.1 - 228 MPa1750 - 33000 psiAverage value: 30.3 MPa Grade Count:95
Tensile Strength, Yield 8.80 - 35.0 MPa1280 - 5080 psiAverage value: 20.9 MPa Grade Count:48
Film Elongation at Break, MD 160 - 1350 %160 - 1350 %Average value: 544 % Grade Count:152
Film Elongation at Break, TD 3.00 - 1100 %3.00 - 1100 %Average value: 583 % Grade Count:146
Elongation at Break 350 - 1700 %350 - 1700 %Average value: 699 % Grade Count:40
Elongation at Yield 8.00 - 11.0 %8.00 - 11.0 %Average value: 9.76 % Grade Count:8
Modulus of Elasticity 0.0200 - 1.35 GPa2.90 - 196 ksiAverage value: 0.836 GPa Grade Count:20
Flexural Modulus 0.660 - 1.50 GPa95.7 - 218 ksiAverage value: 1.07 GPa Grade Count:19
Secant Modulus 0.655 - 1.10 GPa95.0 - 160 ksiAverage value: 0.848 GPa Grade Count:8
Secant Modulus, MD 0.0300 - 100 GPa4.35 - 14500 ksiAverage value: 1.77 GPa Grade Count:106
Secant Modulus, TD 0.0500 - 1.70 GPa7.25 - 247 ksiAverage value: 1.01 GPa Grade Count:105
Izod Impact, Notched 1.47 - 2.94 J/cm2.76 - 5.51 ft-lb/inAverage value: 2.45 J/cm Grade Count:3
Izod Impact, Notched (ISO) 15.0 - 24.0 kJ/m²7.14 - 11.4 ft-lb/in²Average value: 17.8 kJ/m² Grade Count:4
Dart Drop, Total Energy 2.44 - 2.71 J1.80 - 2.00 ft-lbAverage value: 2.53 J Grade Count:3
Puncture Energy 0.722 - 2.14 J0.533 - 1.58 ft-lbAverage value: 1.29 J Grade Count:9
Coefficient of Friction 0.240 - 0.4000.240 - 0.400Average value: 0.284 Grade Count:8
Coefficient of Friction, Static 0.100 - 0.2500.100 - 0.250Average value: 0.175 Grade Count:6
Tear Strength Test 9.80 - 27.49.80 - 27.4Average value: 15.2 Grade Count:15
Elmendorf Tear Strength MD 0.200 - 70.0 g0.200 - 70.0 gAverage value: 24.5 g Grade Count:92
Elmendorf Tear Strength TD 0.800 - 1800 g0.800 - 1800 gAverage value: 332 g Grade Count:90
Elmendorf Tear Strength, MD 0.250 - 70.0 g/micron6.35 - 1780 g/milAverage value: 1.92 g/micron Grade Count:61
Elmendorf Tear Strength, TD 0.800 - 150 g/micron20.3 - 3810 g/milAverage value: 12.6 g/micron Grade Count:62
Dart Drop 1.16 - 30.0 g/micron29.5 - 762 g/milAverage value: 7.65 g/micron Grade Count:50
Dart Drop Test 29.0 - 1000 g0.0639 - 2.20 lbAverage value: 212 g Grade Count:85
Film Tensile Strength at Break, MD 24.1 - 141 MPa3500 - 20500 psiAverage value: 55.5 MPa Grade Count:147
Film Tensile Strength at Break, TD 14.8 - 251 MPa2150 - 36400 psiAverage value: 47.7 MPa Grade Count:146
Heat Seal Strength Initiation Temperature 125 °C257 °FAverage value: 125 °C Grade Count:6
 
Electrical PropertiesMetricEnglishComments
Dielectric Constant 2.332.33Average value: 2.33 Grade Count:3
Dielectric Strength 20.0 kV/mm508 kV/inAverage value: 20.0 kV/mm Grade Count:3
Dissipation Factor 0.0001000.000100Average value: 0.000100 Grade Count:3
 
Thermal PropertiesMetricEnglishComments
Melting Point 72.0 - 270 °C162 - 518 °FAverage value: 133 °C Grade Count:78
Deflection Temperature at 0.46 MPa (66 psi) 59.0 - 64.0 °C138 - 147 °FAverage value: 62.3 °C Grade Count:3
Vicat Softening Point 41.0 - 133 °C106 - 271 °FAverage value: 114 °C Grade Count:69
Softening Point 73.0 - 75.0 °C163 - 167 °FAverage value: 74.2 °C Grade Count:5
Brittleness Temperature -80.0 - -59.0 °C-112 - -74.2 °FAverage value: -69.6 °C Grade Count:21
 
Optical PropertiesMetricEnglishComments
Haze 4.00 - 81.0 %4.00 - 81.0 %Average value: 29.6 % Grade Count:32
Gloss 5.00 - 127 %5.00 - 127 %Average value: 57.3 % Grade Count:30
 
Processing PropertiesMetricEnglishComments
Processing Temperature 20.0 - 260 °C68.0 - 500 °FAverage value: 196 °C Grade Count:23
Melt Temperature 124 - 280 °C255 - 536 °FAverage value: 207 °C Grade Count:65
Die Opening 0.0760 - 0.280 cm0.0299 - 0.110 inAverage value: 0.162 cm Grade Count:10

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Overview of materials for Low Density Polyethylene (LDPE), Film Grade
Overview of materials for Linear Low Density Polyethylene (LLDPE), Film Grade
Overview of materials for High Density Polyethylene (HDPE), Extruded
Overview of materials for High Density Polyethylene (HDPE), Injection Molded
Overview of materials for Medium Density Polyethylene (MDPE), Film Grade

O4007 / 78282

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.