MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
NatureWorks® Ingeo™ 5051X Fiber Grade PLA  (discontinued **)
Categories: Polymer; Renewable/Recycled Polymer; Thermoplastic; Polylactic Acid (PLA) Biopolymer

Material Notes: NatureWorks® PLA polymer 5051X is a thermoplastic fiber-grade resin de-rived primarily from annually renewable resources. Available in pellet form, 5051X is designed for extrusion into mechanically drawn staple fibers using conventional fiber spinning and drawing equipment. NatureWorks® PLA 5051X can be converted into a broad range of disposable fiber products with minimal temperature requirements and is recommended for non-dyed fiber, and injection molded applications. Potential applications for PLA polymer 5051X include Non-woven (spunlace wipes); Injection molded parts

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.24 g/ccASTM D792
Melt Density 1.08 g/cc
@Temperature 230 °C
ASTM D1238
Viscosity Measurement 3.3Relative Viscosity; CD Internal Viscotek Method
 
Mechanical PropertiesOriginal ValueComments
Elongation at Break 10 - 70 %Fiber; ASTM D2256/ASTM D3822
Tenacity 2.50 - 4.00 g/denierASTM D2256/ASTM D3822
 
Thermal PropertiesOriginal ValueComments
Melting Point 145 - 155 °CASTM D3418
Glass Transition Temp, Tg 55.0 - 65.0 °CASTM D3417
Shrinkage <= 8.0 %
@Temperature 120 °C,
Time 600 sec
Hot Air; ASTM D2102
 
Processing PropertiesOriginal ValueComments
Dew Point -35.0 °C
Drying Air Flow Rate >= 0.500 ft³/min (CFM)

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Total PPH 3662 Polypropylene Homopolymer, Fiber Grade, for Staple Fiber, Multifilament Yarns and Slit Tape
NatureWorks® Ingeo™ 6201D Fiber Grade PLA
NatureWorks® Ingeo™ 6060D Fiber Grade PLA
Total PPS 15080 S01 Polypropylene, Homopolymer Fiber Grade
Essentium High Performance PLA Additive Manufacturing Filament

PNATU90 / 103488

Elmet Technologies

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.