System Message
Advertise with MatWeb!
Data sheets for over
180,000
metals, plastics, ceramics, and composites.
HOME
•
SEARCH
•
TOOLS
•
SUPPLIERS
•
FOLDERS
•
ABOUT US
•
FAQ
•
LOG IN
Recently Viewed Materials (most recent at top)
Login
to see your most recently viewed materials here.
Or if you don't have an account with us yet, then
click here to register.
Searches:
Advanced
|
Category
|
Property
|
Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
(Viewing data as-entered.
Click here
to return)
Plenco 08228 Polyester BMC, Compression Molded
Categories:
Polymer
;
Thermoset
;
Filled/Reinforced Thermoset
;
Polyester, TS
;
Thermoset Polyester Glass Filled BMC
Material Notes:
PLENCO 08228 is a glass fiber reinforced polyester bulk molding compound. PLENCO 08228 is formulated for high strength, low warpage, and a wide processing window.
Information supplied by Plenco.
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Original Value
Comments
Density
1.90
g/cc
ASTM D792
Water Absorption
0.070 %
ASTM D570
Linear Mold Shrinkage
0.0037
cm/cm
ASTM D6289
Mechanical Properties
Original Value
Comments
Hardness, Rockwell E
51
ASTM D785
Tensile Strength, Ultimate
56.0
MPa
ASTM D638
Elongation at Break
0.70 %
ASTM D638
Tensile Modulus
13.9
GPa
ASTM D638
Flexural Strength
125
MPa
ASTM D790
Flexural Modulus
13.4
GPa
ASTM D790
Compressive Strength
146
MPa
ASTM D695
Izod Impact, Notched
283
J/m
ASTM D256
Electrical Properties
Original Value
Comments
Volume Resistivity
1.50e+16
ohm-cm
ASTM D247
Dielectric Constant
4.6
@Frequency 1e+6 Hz
ASTM D150
Dielectric Strength
12.2
kV/mm
short time; ASTM D149
Dissipation Factor
0.0080
@Frequency 1e+6 Hz
ASTM D150
Arc Resistance
190
sec
ASTM D495
Comparative Tracking Index
600
V
ASTM D3638
Thermal Properties
Original Value
Comments
CTE, linear
37.0
µm/m-°C
ASTM E831
Maximum Service Temperature, Air
239
°C
Heat Resistance; ASTM D570D
Deflection Temperature at 1.8 MPa (264 psi)
271
°C
ASTM D648
Shrinkage
0.00 %
Post Shrinkage 72 hr, 120ºC; ASTM D6289
Descriptive Properties
Form
BMC
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to go back to viewing the property data in MatWeb's normal format.
PLEM55m4m / 243105
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
info@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.