MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Plenco 08228 Polyester BMC, Compression Molded
Categories: Polymer; Thermoset; Filled/Reinforced Thermoset; Polyester, TS; Thermoset Polyester Glass Filled BMC

Material Notes: PLENCO 08228 is a glass fiber reinforced polyester bulk molding compound. PLENCO 08228 is formulated for high strength, low warpage, and a wide processing window.

Information supplied by Plenco.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.90 g/cc0.0686 lb/in³ASTM D792
Water Absorption 0.070 %0.070 %ASTM D570
Linear Mold Shrinkage 0.0037 cm/cm0.0037 in/inASTM D6289
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell E 5151ASTM D785
Tensile Strength, Ultimate 56.0 MPa8120 psiASTM D638
Elongation at Break 0.70 %0.70 %ASTM D638
Tensile Modulus 13.9 GPa2020 ksiASTM D638
Flexural Strength 125 MPa18100 psiASTM D790
Flexural Modulus 13.4 GPa1940 ksiASTM D790
Compressive Strength 146 MPa21200 psiASTM D695
Izod Impact, Notched 2.83 J/cm5.30 ft-lb/inASTM D256
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.50e+16 ohm-cm1.50e+16 ohm-cmASTM D247
Dielectric Constant 4.6
@Frequency 1e+6 Hz
4.6
@Frequency 1e+6 Hz
ASTM D150
Dielectric Strength 12.2 kV/mm310 kV/inshort time; ASTM D149
Dissipation Factor 0.0080
@Frequency 1e+6 Hz
0.0080
@Frequency 1e+6 Hz
ASTM D150
Arc Resistance 190 sec190 secASTM D495
Comparative Tracking Index 600 V600 VASTM D3638
 
Thermal PropertiesMetricEnglishComments
CTE, linear 37.0 µm/m-°C20.6 µin/in-°FASTM E831
Maximum Service Temperature, Air 239 °C462 °FHeat Resistance; ASTM D570D
Deflection Temperature at 1.8 MPa (264 psi) 271 °C520 °FASTM D648
Shrinkage 0.00 %0.00 %Post Shrinkage 72 hr, 120ºC; ASTM D6289
 
Descriptive Properties
FormBMC

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PLEM55m4m / 243105

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.