MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
PCP-Canada ALCA 5® 5083 Cast Aluminum Mold Plate
Categories: Metal; Nonferrous Metal; Aluminum Alloy; Aluminum Casting Alloy

Material Notes: ALCA5® cast precision plate product has an excellent dimensional stability. The low level of internal stress reduces the plate deformation during and after machining. This high stability leads to cost saving on extra operations such as rough-milling, finishing or re-works. Typical applications are reference plates, machine construction, molds, jigs, and construction equipments.

Information provided by PCP-Canada.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.0960 lb/in³
 
Mechanical PropertiesOriginal ValueComments
Hardness, Brinell 70
Tensile Strength, Ultimate 41000 psi
Tensile Strength, Yield 18000 psi
Elongation at Break 16 %in 2 inches
Modulus of Elasticity 10300 ksi
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.00000640 ohm-cm
 
Thermal PropertiesOriginal ValueComments
CTE, linear 13.2 µin/in-°F
@Temperature 20.0 - 100 °C
Thermal Conductivity 832 BTU-in/hr-ft²-°F
 
Component Elements PropertiesOriginal ValueComments
Aluminum, Al 92.55 - 95.55 %as remainder
Chromium, Cr 0.050 - 0.25 %
Copper, Cu <= 0.10 %
Iron, Fe <= 0.40 %
Magnesium, Mg 4.0 - 4.9 %
Manganese, Mn 0.40 - 1.0 %
Other <= 0.15 %Ti + Zr
Silicon, Si <= 0.40 %
Zinc, Zn <= 0.25 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Vista Metals ATP-5™ Precision Cast Aluminum Plate
Alcoa MIC-6 Aluminum Mold Alloy
Aluminum 6061-T6; 6061-T651
Alpase K100™ Aluminum Plate
Aluminum 5083-H112

NPCPC991 / 133289

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.