MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Vista Metals ATP-5™ Precision Cast Aluminum Plate
Categories: Metal; Nonferrous Metal; Aluminum Alloy; Aluminum Casting Alloy

Material Notes: Used where flatness and dimensional control are critical, such as: computer & electronics, pharmaceuticals, medical testing equipment, packaging machinery, printing machinery, thermoforming tools, machining fixtures, drill jigs, index tables, mold cooling & heating plates, templates, vacuum chucks, food machinery molding plate, automotive and base plates.

Features: Superior Anodizing and Hardening Response; Higher Strength & Elongation; Excellent Weldability; Improved Corrosion Resistance; High Strength to Weight Ratio; Dimensional Stability

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 2.66 g/cc0.0960 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Brinell 7070
Tensile Strength, Ultimate 283 MPa41000 psi
Tensile Strength, Yield 124 MPa18000 psi
Elongation at Break 12 - 15 %12 - 15 %in 2"
Modulus of Elasticity 69.6 GPa10100 ksi
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.0000059 ohm-cm0.0000059 ohm-cm
 
Thermal PropertiesMetricEnglishComments
CTE, linear  23.6 µm/m-°C
@Temperature 20.0 - 100 °C
13.1 µin/in-°F
@Temperature 68.0 - 212 °F
 24.1 µm/m-°C
@Temperature 101 - 200 °C
13.4 µin/in-°F
@Temperature 213 - 392 °F
Thermal Conductivity 140 W/m-K972 BTU-in/hr-ft²-°F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Alcoa MIC-6 Aluminum Mold Alloy
PCP-Canada ALCA 5® 5083 Cast Aluminum Mold Plate
ALIMEX ACP 5080 Aluminum Cast Plate
Overview of materials for Silicone Rubber
ALIMEX ACP 5080R Aluminum Cast Material

NVISTA92 / 131145

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.