MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

(Viewing data as-entered. Click here to return)
Aluminum Silicon Bronze, UNS C64200, M30 Temper, Bar
Categories: Metal; Nonferrous Metal; Copper Alloy; Bronze

Material Notes: Temper: As Hot Extruded

Fabrication Properties: Excellent Suitability – Capacity for Being Hot Formed; Fair Suitability – Brazing, Gas Shielded Arc Welding, Coated Metal Arc Welding, Spot Weld, Seam Weld, Butt Weld; Fair Suitability – Capacity for Being Cold Worked

Common Fabrication Processes: Forging; Hot Forming; Machining

Typical uses: Valve Guides, Automobile Engine; Pole Line Hardware; Bolts; Nuts; Cams; Gears; Valve Bodies; Valve Components; Valve Stems; Hardware

Applicable Specifications: Bar – AMS 4631; Bolts – ASTM F468; Die – Forgings AMS 4631; Forgings, Die (Hot Pressed) – ASME SB283, ASTM B283/B283M; Nuts – ASTM F467; Rod – SAE J463, SAE J461, AMS 4631; Rod, Bar & Shapes - Aluminum Bronze ASME SB150, Aluminum Bronze ASTM B150/B150M, Forgings ASTM B124/B124M; Screws – ASTM F468; Studs – ASTM F468

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.278 lb/in³
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell B 77
@Thickness 19.0 mm
Tensile Strength 75.0 ksi
@Thickness 19.0 mm
Tensile Strength, Yield 35.0 ksi
@Thickness 19.0 mm
0.5% Ext
Elongation at Break 32 %
@Thickness 19.0 mm
Tensile Modulus 16000 ksi
Modulus of Rigidity 6000 ksi
Poissons Ratio 0.33Calculated
Machinability 60 %
Forgeability 80 %
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.0000220 ohm-cm8% IACS
 
Thermal PropertiesOriginal ValueComments
CTE, linear 10.0 µin/in-°F
@Temperature 20.0 - 300 °C
Specific Heat Capacity 0.0900 BTU/lb-°F
Thermal Conductivity 26.0 BTU-in/hr-ft²-°F
Melting Point 1800 - 1840 °F
Solidus 1800 °F
Liquidus 1840 °F
Annealing Point 1100 - 1300 °F
 
Processing PropertiesOriginal ValueComments
Hot-Working Temperature 1300 - 1600 °F
 
Component Elements PropertiesOriginal ValueComments
Aluminum, Al 6.3 - 7.6 %
Arsenic, As >= 0.090 %
Copper, Cu 88.8 - 92.1 %As Balance
Iron, Fe <= 0.30 %
Lead, Pb <= 0.050 %
Manganese, Mn <= 0.10 %
Nickel, Ni <= 0.25 %
Silicon, Si 1.5 - 2.2 %
Tin, Sn <= 0.20 %
Zinc, Zn <= 0.50 %
 
Descriptive Properties
US EPA Registered AntimicrobialYes

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

MC64200x1 / 293049

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.