MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

Aluminum Silicon Bronze, UNS C64200, M30 Temper, Bar
Categories: Metal; Nonferrous Metal; Copper Alloy; Bronze

Material Notes: Temper: As Hot Extruded

Fabrication Properties: Excellent Suitability – Capacity for Being Hot Formed; Fair Suitability – Brazing, Gas Shielded Arc Welding, Coated Metal Arc Welding, Spot Weld, Seam Weld, Butt Weld; Fair Suitability – Capacity for Being Cold Worked

Common Fabrication Processes: Forging; Hot Forming; Machining

Typical uses: Valve Guides, Automobile Engine; Pole Line Hardware; Bolts; Nuts; Cams; Gears; Valve Bodies; Valve Components; Valve Stems; Hardware

Applicable Specifications: Bar – AMS 4631; Bolts – ASTM F468; Die – Forgings AMS 4631; Forgings, Die (Hot Pressed) – ASME SB283, ASTM B283/B283M; Nuts – ASTM F467; Rod – SAE J463, SAE J461, AMS 4631; Rod, Bar & Shapes - Aluminum Bronze ASME SB150, Aluminum Bronze ASTM B150/B150M, Forgings ASTM B124/B124M; Screws – ASTM F468; Studs – ASTM F468

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 7.70 g/cc0.278 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell B 77
@Thickness 19.0 mm
77
@Thickness 0.750 in
Tensile Strength 517 MPa
@Thickness 19.0 mm
75000 psi
@Thickness 0.750 in
Tensile Strength, Yield 241 MPa
@Thickness 19.0 mm
35000 psi
@Thickness 0.750 in
0.5% Ext
Elongation at Break 32 %
@Thickness 19.0 mm
32 %
@Thickness 0.750 in
Tensile Modulus 110 GPa16000 ksi
Modulus of Rigidity 41.4 GPa6000 ksi
Poissons Ratio 0.330.33Calculated
Machinability 60 %60 %
Forgeability 80 %80 %
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.0000220 ohm-cm0.0000220 ohm-cm8% IACS
 
Thermal PropertiesMetricEnglishComments
CTE, linear 18.0 µm/m-°C
@Temperature 20.0 - 300 °C
10.0 µin/in-°F
@Temperature 68.0 - 572 °F
Specific Heat Capacity 0.377 J/g-°C0.0900 BTU/lb-°F
Thermal Conductivity 3.75 W/m-K26.0 BTU-in/hr-ft²-°F
Melting Point 982 - 1000 °C1800 - 1840 °F
Solidus 982 °C1800 °F
Liquidus 1000 °C1840 °F
Annealing Point 593 - 704 °C1100 - 1300 °F
 
Processing PropertiesMetricEnglishComments
Hot-Working Temperature 704 - 871 °C1300 - 1600 °F
 
Component Elements PropertiesMetricEnglishComments
Aluminum, Al 6.3 - 7.6 %6.3 - 7.6 %
Arsenic, As >= 0.090 %>= 0.090 %
Copper, Cu 88.8 - 92.1 %88.8 - 92.1 %As Balance
Iron, Fe <= 0.30 %<= 0.30 %
Lead, Pb <= 0.050 %<= 0.050 %
Manganese, Mn <= 0.10 %<= 0.10 %
Nickel, Ni <= 0.25 %<= 0.25 %
Silicon, Si 1.5 - 2.2 %1.5 - 2.2 %
Tin, Sn <= 0.20 %<= 0.20 %
Zinc, Zn <= 0.50 %<= 0.50 %
 
Descriptive Properties
US EPA Registered AntimicrobialYes

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

MC64200x1 / 293049

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.