MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

(Viewing data as-entered. Click here to return)
Schott FIOLAX® Pro Neutral Glass Tubing
Categories: Ceramic; Glass

Material Notes: Neutral glass tubing, chemically highly resistant

Pharmaceutical primary packaging

The heavy metal content for the elements lead, cadmium, mercury and hexavalent chromium is below 100 ppm.

Information provided by SCHOTT AG.

Vendors: SCHOTT with its Business Unit Tubing offers tailor-made products & services worldwide from more than sixty special glass types for international growth markets such as industrial and environmental technology, electronics, display industry, architecture and design as well as pharmaceuticals. Contact us.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Density 2.32 g/cc
@Temperature 25.0 °C
 
Chemical PropertiesOriginal ValueComments
Acid Class, SR 1DIN 12116
Alkali Class, AR 2ISO 695
 
Thermal PropertiesOriginal ValueComments
CTE, linear 5.20 µm/m-°C
@Temperature 20.0 - 300 °C
ISO 7991
Transformation Temperature, Tg 560 °C
Softening Point 775 °C107.6 dPa . s
Working Point 1170 °C104 dPa . s
Annealing Point 570 °C1013 dPa . s
 
Optical PropertiesOriginal ValueComments
Transmission, Visible 92 - 93 %
@Wavelength 400 - 800 nm,
Thickness 1.00 mm
IR Transmittance 0.0 %
@Wavelength 4500 - 6000 nm,
Thickness 1.00 mm
 24 %
@Thickness 1.00 mm,
Wavelength 2800 nm
 <= 30 %
@Wavelength >=3500 nm,
Thickness 1.00 mm
 60 %
@Thickness 1.00 mm,
Wavelength 3300 nm
 90 - 93 %
@Wavelength 800 - 2500 nm,
Thickness 1.00 mm
 
Component Elements PropertiesOriginal ValueComments
Al2O3 7 %
B2O3 11 %
CaO <= 1 %
K2O <= 1 %
Na2O 7 %
SiO2 73 %
 
Descriptive Properties
Glasses in Laboratory ApparatusType I Class BASTM E 438
Hydrolytic ResistanceClass HGA 1ISO 720
 Class HGB 1ISO 719
 Class HGB 1YBB00362004-2015
 fulfilledJP
 Type IPh. Eur.
 Type IUSP
 Type IYBB00252003-2015

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

CSGS910c / 322919

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.