MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Schott FIOLAX® Pro Neutral Glass Tubing
Categories: Ceramic; Glass

Material Notes: Neutral glass tubing, chemically highly resistant

Pharmaceutical primary packaging

The heavy metal content for the elements lead, cadmium, mercury and hexavalent chromium is below 100 ppm.

Information provided by SCHOTT AG.

Vendors: SCHOTT with its Business Unit Tubing offers tailor-made products & services worldwide from more than sixty special glass types for international growth markets such as industrial and environmental technology, electronics, display industry, architecture and design as well as pharmaceuticals. Contact us.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 2.32 g/cc
@Temperature 25.0 °C
0.0838 lb/in³
@Temperature 77.0 °F
 
Chemical PropertiesMetricEnglishComments
Acid Class, SR 11DIN 12116
Alkali Class, AR 22ISO 695
 
Thermal PropertiesMetricEnglishComments
CTE, linear 5.20 µm/m-°C
@Temperature 20.0 - 300 °C
2.89 µin/in-°F
@Temperature 68.0 - 572 °F
ISO 7991
Transformation Temperature, Tg 560 °C1040 °F
Softening Point 775 °C1430 °F107.6 dPa . s
Working Point 1170 °C2140 °F104 dPa . s
Annealing Point 570 °C1060 °F1013 dPa . s
 
Optical PropertiesMetricEnglishComments
Transmission, Visible 92 - 93 %
@Wavelength 400 - 800 nm,
Thickness 1.00 mm
92 - 93 %
@Wavelength 400 - 800 nm,
Thickness 0.0394 in
IR Transmittance  0.0 %
@Wavelength 4500 - 6000 nm,
Thickness 1.00 mm
0.0 %
@Wavelength 4500 - 6000 nm,
Thickness 0.0394 in
 24 %
@Thickness 1.00 mm,
Wavelength 2800 nm
24 %
@Thickness 0.0394 in,
Wavelength 2800 nm
 <= 30 %
@Wavelength >=3500 nm,
Thickness 1.00 mm
<= 30 %
@Wavelength >=3500 nm,
Thickness 0.0394 in
 60 %
@Thickness 1.00 mm,
Wavelength 3300 nm
60 %
@Thickness 0.0394 in,
Wavelength 3300 nm
 90 - 93 %
@Wavelength 800 - 2500 nm,
Thickness 1.00 mm
90 - 93 %
@Wavelength 800 - 2500 nm,
Thickness 0.0394 in
 
Component Elements PropertiesMetricEnglishComments
Al2O3 7 %7 %
B2O3 11 %11 %
CaO <= 1 %<= 1 %
K2O <= 1 %<= 1 %
Na2O 7 %7 %
SiO2 73 %73 %
 
Descriptive Properties
Glasses in Laboratory ApparatusType I Class BASTM E 438
Hydrolytic ResistanceClass HGA 1ISO 720
 Class HGB 1ISO 719
 Class HGB 1YBB00362004-2015
 fulfilledJP
 Type IPh. Eur.
 Type IUSP
 Type IYBB00252003-2015

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

CSGS910c / 322919

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.