MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Lanxess STABAXOL® P 200 Antihydrolysis agent
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: Function: Antihydrolysis agent for polyester polyurethanes and thermoplastic polyester polyurethanes (TPU).

Product information: Stabaxol® P 200 is an antihydrolysis agent for:

  • hot casting polyester polyurethanes,
  • polyurethane shoe-sole systems based on polyester polyols
  • polyester polyurethane adhesives,
  • thermoplastic polyester polyurethanes (TPU) as well
It is recommended to add 1.0 - 4.0 p.b.w. Stabaxol® P 200 on 100 p.b.w. of the polyol component. However, prior tests should always be carried out to determine the most suitable dosage. Upon processing Stabaxol® P 200 is normally being dissolved in the polyester polyol; alternatively, it may be added to the pre-polymers (only with terminal OH groups) or may be added directly into the mixing head in case of cast systems.

Information provided by Lanxess.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.10 g/cc
Viscosity 1000 - 6000 cP
 
Thermal PropertiesOriginal ValueComments
Melting Point <= 5.00 °CFreezing Point
 
Processing PropertiesOriginal ValueComments
Shelf Life 12.0 Month
 
Descriptive Properties
Appearanceviscous. bright yellow liquid
Color<25Iodine color
Content>6%Carbodiimide
Specifications13 mg KOH/gOH-value, theoretical

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PLANY9068 / 209459

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.