Function: Antihydrolysis agent for polyester polyurethanes and thermoplastic polyester polyurethanes (TPU). Product information: Stabaxol® P 200 is an antihydrolysis agent for: - hot casting polyester polyurethanes,
- polyurethane shoe-sole systems based on polyester polyols
- polyester polyurethane adhesives,
- thermoplastic polyester polyurethanes (TPU) as well
It is recommended to add 1.0 - 4.0 p.b.w. Stabaxol® P 200 on 100 p.b.w. of the polyol component. However, prior tests should always be carried out to determine the most suitable dosage. Upon processing Stabaxol® P 200 is normally being dissolved in the polyester polyol; alternatively, it may be added to the pre-polymers (only with terminal OH groups) or may be added directly into the mixing head in case of cast systems.Information provided by Lanxess. |