MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Chemically Resistant adhesives

(Viewing data as-entered. Click here to return)
CoorsTek PolyGlyde™ 5400 Self-Lubricating Seal
Categories: Polymer

Material Notes: PolyGlyde seals offer low heat generation in high-friction and high-stress environments. These seals provide superior performance over traditional carbon materials: runs cooler – even in dry-running situations, leak-tight material, greater durability, less wear debris – runs cleaner, broader resistance to chemical attack, suitable for fluid and gas applications, lapping of seal face not necessary, and exceptionally stable.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 2.01 g/ccASTM-D792
Deformation 5.9 %
@Pressure 13.8 MPa,
Temperature 25.6 °C
24 hrs.; ASTM-D621
 9.9 %
@Pressure 4.14 MPa,
Temperature 260 °C
24 hrs.; ASTM-D621
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Ultimate 1800 psiASTM-D1457
Elongation at Break 60 %ASTM-D1457
Flexural Strength 2500 psiASTM-F417
Flexural Modulus 1700 psiASTM-D790
Compressive Strength 7000 psiASTM-C773
 
Thermal PropertiesOriginal ValueComments
CTE, linear 8.00 µin/in-°FASTM-D696
Thermal Conductivity 5.60 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 260 °C
 
Descriptive Properties
ColorBlack

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Sandvik Kanthal 145 R 15 Thermostatic bimetal
Overview of materials for Stainless Steel
Dicronite® Tungsten Disulfide Dry Lubricant
Daelim H&L Plavis-N ISO Unfilled Aromatic Polyimide Bearing
BryCoat WS2 Tungsten Disulfide Coating

PCOOR925 / 104629

Chemically Resistant adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.