MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
DuPont Mobility and Materials Zytel® RS 30G30HSL BK038A Nylon 610  (discontinued **)
Categories: Polymer; Renewable/Recycled Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 610 (PA610)

Material Notes: 30% Glass Reinforced Renewably Sourced Polyamide 610 Developed for Extrusion

While this product line has been acquired by Celanese, this specific grade had been disconued while still a DuPont product so it is listed here as a discontinued DuPont product.

Key Words: PA610-GF30
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.16 g/cc
 1.31 g/ccDAM; ISO 1183
Moisture Absorption 1.20 %
@Thickness 2.00 mm
DAM; Sim. to ISO 62
Viscosity 360000 cP
@Temperature 250 °C
DAM; @ 1000 sec-1; ISO 11443
 94180 cP
@Shear Rate 5000 1/s,
Temperature 280 °C
ISO 11403-1 -2
 116100 cP
@Shear Rate 5000 1/s,
Temperature 260 °C
ISO 11403-1 -2
 130300 cP
@Shear Rate 5000 1/s,
Temperature 250 °C
ISO 11403-1 -2
 341600 cP
@Shear Rate 500 1/s,
Temperature 280 °C
ISO 11403-1 -2
 455400 cP
@Shear Rate 500 1/s,
Temperature 260 °C
ISO 11403-1 -2
 527100 cP
@Shear Rate 500 1/s,
Temperature 250 °C
ISO 11403-1 -2
Linear Mold Shrinkage, Flow 0.0020 cm/cmDAM; ISO 294-4 2577
Linear Mold Shrinkage, Transverse 0.0070 cm/cmDAM; ISO 294-4 2577
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 130 MPa50%RH; ISO 527-1/-2
 140 MPaDAM; ISO 527-1/-2
Elongation at Break 3.6 %DAM; ISO 527-1/-2
 6.5 %50%RH; ISO 527-1/-2
Tensile Modulus 6800 MPa50%RH; ISO 527-1/-2
 8100 MPaDAM; ISO 527-1/-2
Izod Impact, Notched (ISO) 12.0 kJ/m²DAM; ISO 180/1A
 16.0 kJ/m²50%RH; ISO 180/1A
Charpy Impact Unnotched 80.0 kJ/m²DAM; ISO 179/1eU
 95.0 kJ/m²50%RH; ISO 179/1eU
Charpy Impact, Notched 11.0 kJ/m²DAM; ISO 179/1eA
 15.0 kJ/m²50%RH; ISO 179/1eA
 
Thermal PropertiesOriginal ValueComments
Specific Heat Capacity 2.28 J/g-°C
Thermal Conductivity 0.260 W/m-Kof melt
Melting Point 225 °CDAM; 10°C/min; ISO 11357-1/-3
Deflection Temperature at 1.8 MPa (264 psi) 207 °CDAM; ISO 75-1/-2
Glass Transition Temp, Tg 50.0 °CDAM; 10°C/min; ISO 11357-1/-2
 
Descriptive Properties
AdditivesLubricants
 Release agent
Delivery formPellets
Part Marking Code>PA610-GF30<ISO 11469
ProcessingInjection Molding
Regional AvailabilityAsia Pacific
 Europe
 Global
 Near East/Africa
 North America
 South and Central America
Resin IdentificationPA610-GF30ISO 1043
Special characteristicsHeat stabilized or stable to heat

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Akro-Plastic Akromid® A3 GF 25 (2420) PA 6.6 Conditioned, 25% Glass Filled
Avient Edgetek® NL-20GF/000 BLACK Polyamide 612 (Nylon 612)
Evonik Vestamid® X7099 nf (dry properties) Nylon 612
Overview of materials for Nylon 610
RTP Company RTP 203 B Nylon 6/10 (PA), Glass Fiber

PZDSY5474 / 161301

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.