MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Dow AFFINITY™ SM 1300G Polyolefin Plastomer (POP)
Categories: Polymer; Thermoplastic; Polyolefin

Material Notes: AFFINITY™ SM 1300G is an ethylene alpha-olefin resin for Injection Molding is produced via INSITE™ Technology from Dow Plastics. The resin offers excellent performance in durable injection molded industrial and consumer goods and compression molded closure liners or gaskets.

Information provided by Dow

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.902 g/ccASTM D792
Thickness 125 milinjection molded
Melt Flow 30 g/10 minASTM D1238
Slip Level 600 ppm
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Ultimate 1326 psicrosshead speed 20 in./min; ASTM D638
Tensile Strength, Yield 598 psicrosshead speed 20 in./min; ASTM D638
Elongation at Break 624 %crosshead speed 20 in./min; ASTM D638
Flexural Modulus 10280 psiASTM D790
2% Secant Modulus 10280 psiASTM D790
Izod Impact, Notched 1.00 ft-lb/in
@Temperature -50.0 °C
ASTM D256
 4.00 ft-lb/in
@Temperature 23.0 °C
ASTM D256
 5.00 ft-lb/in
@Temperature 0.000 °C
ASTM D256
 9.00 ft-lb/in
@Temperature -20.0 °C
ASTM D256
 
Thermal PropertiesOriginal ValueComments
Melting Point 98.0 °CDow Method (DSC)
Vicat Softening Point 79.0 °CASTM D1525

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Dow AFFINITY™ PT 1409 Polyolefin Plastomer (POP)
Dow AFFINITY™ GA 1900 Polyolefin Plastomer (POP)
Dow AFFINITY™ EG 8200G Ethylene alpha-olefin copolymer
Dow AFFINITY™ PT 1450G1 Ethylene alpha-olefin resin
Dow AFFINITY™ EG 8100 Polyolefin Elastomer

PDOW1179 / 30397

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.