Dow AFFINITY™ PT 1409 Polyolefin Plastomer (POP)
Categories:
Polymer
;
Thermoplastic
;
Polyolefin
Material Notes:
AFFINITY™ PT 1409 Polyolefin Plastomer (POP) is produced via INSITE™ Technologies from Dow Plastics. Resin blended with 20 wt% LDPE to improve extrusion coating performance.
Information provided by Dow
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Metric
English
Comments
Density
0.911
g/cc
0.0329
lb/in³
ASTM D792
Thickness
>=
6.35
microns
>=
0.250
mil
Coating Thickness; Extrusion Coating Processability; Dow Method
Melt Index of Compound
6.0
g/10 min
6.0
g/10 min
ASTM D1238
Neck In
11.4
cm
4.49
in
610°F and 1.0 mil; Extrusion Coating Processability; Dow Method
Coating Weight
>=
6.08
g/m²
>=
3.80
lb/ream
Extrusion Coating Processability; Dow Method
Thermal Properties
Metric
English
Comments
Melting Point
108
°C
226
°F
Dow Method (DSC)
Vicat Softening Point
91.0
°C
196
°F
ASTM D1525
Processing Properties
Metric
English
Comments
Melt Temperature
288
-
321
°C
550
-
610
°F
Extrusion Coating Processability
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to view all the property values for this datasheet as they were originally entered into MatWeb.
Users viewing this material also viewed the following:
Dow AFFINITY™ PT 1450G1 Ethylene alpha-olefin resin
Dow AFFINITY™ SM 1300G Polyolefin Plastomer (POP)
Dow AFFINITY™ GA 1900 Polyolefin Plastomer (POP)
Dow AFFINITY™ EG 8200G Ethylene alpha-olefin copolymer
Dow AFFINITY™ EG 8185 Polyolefin Plastomer (POP)
PDOW1177 / 30395
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
info@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.