MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Morgan Advanced Ceramics Sintox ™ FA Ballistic Mac-A950R Aluminum Oxide Ceramic
Categories: Ceramic; Oxide; Aluminum Oxide

Material Notes: Alumina ceramic with a minimum Al2O3 content of 95.0% (typically 96%). This lightweight hard-faced material is especially formulated for ballistic applications. (MTC pioneered monolithic ceramic tiles that are now the accepted standard for body armour.)

Prime Features:

  • Excellent ballistic properties
  • High mechanical strength
  • Can be moulded as double or single curvature monolithic tiles for ‘ergonomic’ body armour
  • Weight savings of up to 10% in comparison with traditional ballistic tile materials
Typical Applications:
  • Ergonomic body armour for defence and security services
  • Armour tiles for battlefield vehicles
Production Capabilities:
  • Body armour — single and double curvature monolithic tiles, groin tiles, and smaller mosaic tiles
  • Vehicle armour — standard tiles, tile kits, and prototypes to customer requirements
  • Prototype, batch and volume production

Information provided by Morgan Advanced Materials

Key Words: Mac-A950R
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Bulk Density 3.74 g/cc0.135 lb/in³
Open Porosity 0.00 %0.00 %fully dense, % nominal, apparent
Grain Size 4.0 µm4.0 µm
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell HR45N 7878
Hardness, Vickers 12.5
@Load 0.500 kg
12.5
@Load 1.10 lb
[GPa]
Modulus of Elasticity 320 GPa46400 ksi
Flexural Strength 350 MPa50800 psi3-point
Compressive Strength 2000 MPa290000 psi
Poissons Ratio 0.230.23
Fracture Toughness 4.60 MPa-m½4.19 ksi-in½KIC(SENB)
Shear Modulus 130 GPa18900 ksitime of flight method
 
Component Elements PropertiesMetricEnglishComments
Al2O3 >= 95 %>= 95 %
 
Descriptive Properties
Colorpink

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
AISI Type 304L Stainless Steel
Aluminum 2014-O
AK Steel ULTRALUME® Press Hardenable Carbon Steel
ERG Aerospace Duocel® Aluminum Metal Foam
ATI Allegheny Ludlum Stainless Steel Chromium-Nickel Type 304L, 60% Cold Rolled (UNS S30403)

CMORF5021 / 200259

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.