MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

AK Steel ULTRALUME® Press Hardenable Carbon Steel
Categories: Metal; Ferrous Metal; Carbon Steel

Material Notes: ULTRALUME Press Hardenable Steel (PHS) is an Advanced High Strength Steels (AHSS). Aluminized Type 1 ULTRALUME PHS is intended for automotive steel applications where high strength, design flexibility and collision protection are paramount. Blanks produced from ULTRALUME PHS are heated in a furnace at 900° to 950 °C to bring the steel into the austenitic temperature range. The blank is then transferred to a hot forming press where the hot steel is formed into complex shapes. The steel cools rapidly inside the water-cooled dies and undergoes a phase transformation from austenite to a high strength phase – martensite. This rapid cooling, or quenching, increases the tensile strength of the steel from approximately 600 MPa to 1,400 MPa and higher. Since the steel is held in the dies during cooling, thermo-distortion and springback are avoided.
ULTRALUME PHS is continuously hot dip coated on both sides of the steel. The aluminum coating bath contains approximately 91% aluminum and 9% silicon. The metallic coating is metallurgically bonded to the steel substrate and protects the steel surface against decarburization and oxidation during hot stamping. As a result, the shot blasting operation required for hot-stamped, uncoated steel parts is eliminated.

Information provided by AK Steel.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Ultimate 632 MPa91700 psiLongitudinal
 650 MPa94300 psiTransverse
Tensile Strength, Yield  438 MPa
@Strain 0.2 %
63500 psi
@Strain 0.2 %
Longitudinal
 465 MPa
@Strain 0.2 %
67400 psi
@Strain 0.2 %
Transverse
Elongation at Break 22 %22 %Transverse
 26 %26 %Longitudinal
 
Component Elements PropertiesMetricEnglishComments
Boron, B 0.0030 %0.0030 %
Carbon, C 0.22 %0.22 %
Chromium, Cr 0.20 %0.20 %
Iron, Fe 98.127 %98.127 %Balance
Manganese, Mn 1.2 %1.2 %
Silicon, Si 0.25 %0.25 %
 
Descriptive Properties
n Value (10% -Ult)0.145Transverse
 0.151Longitudinal

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
SSAB Tunnplat Docol® 1000 DP High-strength Steel
SSAB Tunnplat Docol® 1400 DP High-strength Steel
Crucible Steel CPM® 4V® Tool Steel
AISI 1045 Steel, as cold drawn, 22-32 mm (0.875-1.25 in) round
SSAB Tunnplat Docol® 800 DP High-strength Steel

NAKS224 / 140770

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.