MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Phillips 66 Steaval D-150 ISO Grade 460
Categories: Fluid; Lubricant

Material Notes: Steaval D-150 is a heavy, non-compounded paraffinic mineral oil developed for steam cylinder and valve lubrication in applications that require a non-emulsifying oil, or where the steam is superheated. It also may be used in applications where an ISO VG 460 or SAE 140 straight mineral gear oil is required. Steaval D-150 is manufactured from highly refined, high-viscosity paraffinic base stocks and contains no additives. It forms a tough film on metal surfaces to protect against wear

Applications:

  • Steam cylinders and valves in applications that require a non-compounded oil, or where the steam is superheated
  • Paper mill calendar roll bearings
  • Steel mill roll neck bearings
  • Rack and pinion gears and heavy mill gears
  • Applications that require an ISO VG 460 or SAE 140 straight mineral gear oil
Features/Benefits:
  • High film strength
  • Good retention on metal surfaces
  • Noncorrosive to bronze or brass

Information provided by Phillips 66 Lubricants.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 0.890 g/cc
Density 7.41 lb/gal
Viscosity Measurement 96Index
Saybolt Viscosity at 100°F 2645 SUS
Saybolt Viscosity at 210°F 157 SUS
Kinematic Viscosity at 40°C (104°F) 493 cSt
Kinematic Viscosity at 100°C (212°F) 32 cSt
ASTM Color 5.0ASTM D1500
 
Chemical PropertiesOriginal ValueComments
Total Acid Number 0.020[mg KOH/g]; ASTM D974
 
Thermal PropertiesOriginal ValueComments
Pour Point -12.0 °C
Flash Point 312 °CCOC
 
Descriptive Properties
Carbon Residue0.51%ASTM D524
Copper Corrosion1aASTM D130

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

WCON5233 / 198486

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.