Steaval D-150 is a heavy, non-compounded paraffinic mineral oil developed for steam cylinder and valve lubrication in applications that require a non-emulsifying oil, or where the steam is superheated. It also may be used in applications where an ISO VG 460 or SAE 140 straight mineral gear oil is required. Steaval D-150 is manufactured from highly refined, high-viscosity paraffinic base stocks and contains no additives. It forms a tough film on metal surfaces to protect against wear Applications: - Steam cylinders and valves in applications that require a non-compounded oil, or where the steam is superheated
- Paper mill calendar roll bearings
- Steel mill roll neck bearings
- Rack and pinion gears and heavy mill gears
- Applications that require an ISO VG 460 or SAE 140 straight mineral gear oil
Features/Benefits:- High film strength
- Good retention on metal surfaces
- Noncorrosive to bronze or brass