MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

Thermal Ceramics Unifelt 3000M
Categories: Ceramic; Oxide; Aluminum Oxide

Material Notes: Unifelt Veneering modules, 3000 (HT), 3000 M, XT are made from a blend of high-temperature Kaowool fiber and Saffil alumina fiber. The modules are fabricated into blocks, 12" by 12" (305 mm x 305 mm) using pre-cut Unifelt boards turned edge-grain and glued together.

Unifelt veneering modules are part of the Unisystem family of products. They can be applied over a variety of surfaces including refractory castable, monolithic plastics, high-temperature IFB and ceramic fiber modules. K-Bond mortar, a high-temperature air setting mortar is used to attach the Unifelt modules. Unikote S surface coating is then applied over the module hot face to provide greater thermal stability and chemical attack resistance. A typical application would be stack-on-stack design linings over new ceramic fiber weld-on modules.

Features:

  • 12" x 12" (305 mm x 305 mm) blocks of ceramic fiber insulation
  • Easily installed over existing refractory surface
  • Improves furnace efficiency without replacing a serviceable refractory lining
  • Good insulating properties
  • Excellent thermal stability
  • Applications:

  • Forge furnaces
  • Crucible furnace
  • Rotary hearth furnace
  • Holding furnace
  • Heat treating furnace
  • Pusher reheat furnace
  • Ceramic kiln
  • Information provided by Thermal Ceramics

    Data has not been recently verified. Please contact manufacturer for current information.

    Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
     
    Physical PropertiesMetricEnglishComments
    Density 0.112 g/cc0.00405 lb/in³
    Loss On Ignition 6.0 %6.0 %
     
    Thermal PropertiesMetricEnglishComments
    Thermal Conductivity  0.0879 W/m-K
    @Temperature 260 °C
    0.610 BTU-in/hr-ft²-°F
    @Temperature 500 °F
    ASTM C201
     0.166 W/m-K
    @Temperature 538 °C
    1.15 BTU-in/hr-ft²-°F
    @Temperature 1000 °F
    ASTM C201
     0.303 W/m-K
    @Temperature 816 °C
    2.10 BTU-in/hr-ft²-°F
    @Temperature 1500 °F
    ASTM C201
     0.522 W/m-K
    @Temperature 1090 °C
    3.62 BTU-in/hr-ft²-°F
    @Temperature 2000 °F
    ASTM C201
    Maximum Service Temperature, Air 1540 °C2800 °FContinuous
     1650 °C3000 °FRating
     
    Component Elements PropertiesMetricEnglishComments
    Al2O3 62 %62 %
    SiO2 38 %38 %
     
    Descriptive Properties
    Other Element Contenttraces

    Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

    Users viewing this material also viewed the following:
    Morgan Advanced Ceramics Kaowool HP Veneering Module Thermal Ceramic
    Morgan Advanced Ceramics Kaowool Ceramic Felt 1260 Thermal Ceramic
    Morgan Advanced Ceramics Kaowool C Veneering Module Thermal Ceramic
    Morgan Advanced Ceramics Green Glass Paper Thermal Ceramic
    Morgan Advanced Ceramics Ceramic Fiber Papers STD Paper Ceramic Fiber

    CTHERM092 / 2412

    Free Trade Publications, Click Here!
    Free Trade Publications, Click Here!

    Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

    The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.