System Message
Advertise with MatWeb!
Data sheets for over
180,000
metals, plastics, ceramics, and composites.
HOME
•
SEARCH
•
TOOLS
•
SUPPLIERS
•
FOLDERS
•
ABOUT US
•
FAQ
•
LOG IN
Recently Viewed Materials (most recent at top)
Login
to see your most recently viewed materials here.
Or if you don't have an account with us yet, then
click here to register.
Searches:
Advanced
|
Category
|
Property
|
Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
(Viewing data as-entered.
Click here
to return)
NOVA Chemicals Sclair® 19C Homopolymer HDPE Film Resin
Categories:
Polymer
;
Film
;
Thermoplastic
;
Polyethylene (PE)
;
High Density (HDPE)
;
High Density Polyethylene (HDPE), Film Grade
Material Notes:
Film Properties. Features: Good stiffness, good barrier, high clarity, narrow MWD.
Applications:
Lamination, co-extrusion.
Data provided by the manufacturer.
Key Words:
High Density Polyethylene
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Original Value
Comments
Density
0.958
g/cc
ASTM D792
Water Vapor Transmission
2.64
g/m²/day
ASTM F1249
Oxygen Transmission Rate
1488
cc/m²/day
ASTM D3985
Thickness
38.0
microns
Melt Flow
0.95
g/10 min
@Load 2.16 kg,
Temperature 190 °C
ASTM D1238
Mechanical Properties
Original Value
Comments
Hardness, Shore D
68
ASTM D2240
Film Tensile Strength at Yield, MD
25.0
MPa
ASTM D882
Film Tensile Strength at Yield, TD
27.0
MPa
ASTM D882
Film Elongation at Break, MD
560 %
ASTM D882
Film Elongation at Break, TD
890 %
ASTM D882
Secant Modulus, MD
0.840
GPa
ASTM D882
Secant Modulus, TD
1.18
GPa
ASTM D882
Coefficient of Friction
>= 0.40
ASTM D1894
Elmendorf Tear Strength, MD
0.630
g/micron
ASTM D1922
Elmendorf Tear Strength, TD
18.7
g/micron
ASTM D1922
Dart Drop
1.16
g/micron
F 50; ASTM D1709/A
Film Tensile Strength at Break, MD
42.0
MPa
ASTM D882
Film Tensile Strength at Break, TD
40.0
MPa
ASTM D882
Thermal Properties
Original Value
Comments
Vicat Softening Point
131
°C
ASTM D1525
Optical Properties
Original Value
Comments
Haze
36 %
ASTM D1003
Gloss
23 %
45°; ASTM D2457
Processing Properties
Original Value
Comments
Melt Temperature
220
-
230
°C
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to go back to viewing the property data in MatWeb's normal format.
Users viewing this material also viewed the following:
Chevron Phillips Marlex® 9659 HDPE Blown Film Resin
Chevron Phillips Marlex® 9656 HDPE Blown Film Resin
Overview of materials for High Density Polyethylene (HDPE), Film Grade
LyondellBasell Alathon L4550 High Denisty Polyethylene
LyondellBasell Alathon L 5645 High Denisty Polyethylene
PEHN0T / 35542
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
webmaster@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.