MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Morgan Advanced Ceramics Alumor 60 Thermal Ceramic
Categories: Ceramic; Oxide

Material Notes: Andalusite. Hydraulic bond. A 1650°C grade, low cement castable exhibiting high strengths, good abrasion resistance and excellent resistance to thermal shock. Contains a non-wetting additive for enhanced resistance to aluminium penetration and corundum growth.

Typical applications: Suitable in molten aluminium contact for melting and holding furnaces.

Information provided by Morgan Advanced Materials

Key Words: Thermal Ceramics
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Bulk Density 2.515 g/ccdried to 110°C
Grain Size <= 6000 µm
 
Mechanical PropertiesOriginal ValueComments
Compressive Strength 50.0 - 80.0 MPa
@Treatment Temp. 110 °C
Cold Crushing Strength
 50.0 - 80.0 MPa
@Treatment Temp. 815 °C
Cold Crushing Strength
 60.0 - 90.0 MPa
@Treatment Temp. 1000 °C
Cold Crushing Strength
 100 - 150 MPa
@Treatment Temp. 1650 °C
Cold Crushing Strength
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air <= 1650 °C
Shrinkage -0.700 - 0.70 %
@Treatment Temp. 1650 °C
 -0.100 - 0.10 %
@Treatment Temp. 1000 °C
 0.00 - 0.20 %
@Treatment Temp. 110 °C
 0.00 - 0.20 %
@Treatment Temp. 815 °C
 
Component Elements PropertiesOriginal ValueComments
Al2O3 59 %
CaO 1.6 %
Fe2O3 1.0 %
K2O+Na2O 0.40 %Na2O + K2O
SiO2 37 %
TiO2 0.70 %
 
Descriptive Properties
Net Material Required (kg/m³)2480
Water Addition6-6.5 % by weight, 1.5-1.625 L per bag, 25 kg bag weight.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

CMORF6321 / 203105

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.