MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Carpenter O6 Graphitic Tool Steel (AISI O6)
Categories: Metal; Ferrous Metal; Tool Steel; Cold Work Steel; Oil-Hardening Steel

Material Notes: Carpenter O6 is an oil-hardening tool steel designed for cold work applications. It is designed to have free graphite in the microstructure. This free graphite is responsible for the excellent machining characteristics of this grade. It is available as a DeCarb-Free product. DCF bars have been cold finished in the mill, eliminating the need for bar bark removal.

Applications: Blanking dies, Drawing dies, Forming dies, Punches, Hobs for nonferrous metals, Gauges, Cams, Bushings, Mandrels, Piercing dies, Pneumatic hammers, Spinning tools, Stamps, Taps, Edging and metal forming rolls, Jewelers anvils, Rotary slitting cutters, Marking tools, Wear plates

Information provided by Carpenter Technology Corporation.

Key Words: UNS T31506
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 7.67 g/cc
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell C 31Tempered at 1200°F
 65As hardened
 
Thermal PropertiesOriginal ValueComments
CTE, linear 12.48 µm/m-°C
@Temperature 25.0 - 250 °C
 13.17 µm/m-°C
@Temperature 25.0 - 350 °C
 13.86 µm/m-°C
@Temperature 25.0 - 500 °C
 
Component Elements PropertiesOriginal ValueComments
Carbon, C 1.45 %
Iron, Fe 96.45 %As Balance
Manganese, Mn 0.85 %
Molybdenum, Mo 0.25 %
Silicon, Si 1.0 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Crucible Steel HALGRAPH® Tool Steel, AISI O6
AISI Type O6 Tool Steel
AISI Type O1 Oil-hardening Tool Steel, oil quenched at 800°C, tempered at 425°C
Carpenter Stentor® Alloy Tool Steel (Oil-Hard) (AISI 02)
Crucible Steel KETOS® Tool Steel, AISI O1

NCARN24 / 15863

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.