MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Geon® Performance Solutions X150-206-147-2 Vinyl Compound - Rigid (RPVC)  (discontinued **)
Categories: Polymer; Thermoplastic; Vinyl (PVC)

Material Notes:

Description/Features:

  • Thermoformable

Applications:

  • Interior

Processing Method:

  • Extrusion-Sheet
  • Extrusion-Twin Screw

Information provided by PolyOne Corporation.

Geon Performance Solutions was created from PolyOne in 2019.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.4329 g/cc1.4329 g/ccASTM D792
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 82.582.5Instantaneous; ASTM D2240
Tensile Strength, Yield 44.2 MPa6410 psiType 1 - Rigids, 0.2 in/min; ASTM D638
Tensile Modulus 2.83 GPa411 ksiType 1 - Rigids, 0.2 in/min; ASTM D638
Flexural Strength 80.0 MPa11600 psiASTM D790
Flexural Modulus 2.85 GPa414 ksiASTM D790
Izod Impact, Notched 1.52 J/cm
@Thickness 3.17 mm
2.84 ft-lb/in
@Thickness 0.125 in
Method A, Compression Molded; ASTM D256
Dart Drop Total Energy 64.1 J/cm0.120 ft-lb/milProcedure A, 0.125 in Conical Dart, 73°F (23°C); ASTM D4226
 182 J/cm0.340 ft-lb/milProcedure B, 0.125 in Conical Dart, 73°F (23°C); ASTM D4226
 
Thermal PropertiesMetricEnglishComments
CTE, linear 67.1 µm/m-°C
@Temperature 20.0 °C
37.3 µin/in-°F
@Temperature 68.0 °F
ASTM D696
Deflection Temperature at 1.8 MPa (264 psi) 73.00 °C163.4 °FUnannealed, 0.125 in bars; ASTM D648
 
Processing PropertiesMetricEnglishComments
Melt Temperature 193 - 204 °C380 - 400 °FExtrusion
 
Descriptive Properties
Cell Classification D178413354ASTM D1784
Product FormPowder

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Axiall 3121 Rigid PVC, Extrusion
Axiall 7555 Rigid PVC, Extrusion, White
Axiall 5006 Rigid PVC, Extrusion, White
Axiall 3101 Rigid PVC, Extrusion
Geon® Performance Solutions x150-206-14702 Vinyl Compound - Rigid (RPVC)

PH1PO2380 / 44522

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.